| 一种性能优异的低成本定向凝固镍基高温合金DZ417G |
| 郭建亭 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
郭建亭 . 一种性能优异的低成本定向凝固镍基高温合金DZ417G[J]. 金属学报, 2002, 38(11): 1163-1174 .
[1] Jin Z, Ma S J. Acta Metall Sin, 1974; 10: 3(金 柱,马实基.金属学报,1974;10:3) [2] Zhu Y X, Zhang S N, Zhang T X, Zhang J H, Hu Z Q, Xie C X, Shi C X. In: Antolovich S P, Stusrud R W, Mackay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds, Superalloy 199S, Warrendale, PA: TMS, 1992: 145 [3] Li H, Wang S H, Guo J T, Yin W M, Tan M H, Lai W H. Acta Metall Sin, 1995; 31(Suppl): S316(李 辉,王淑荷,郭建亭,殷为民,谭明晖,赖万慧.金属学报,1995 31(Suppl):S316) [4] Li Y A, Tang Y J, Guo J T, Tian W M, Zheng Q, Zhao J R, Guan H R, Hu Z Q. Acta Metall Sin, 1995; 31(Suppl): S320(李英敖,唐亚俊,郭建亭,田为民,郑 启,赵及仁,管恒荣,胡壮麒,金属学报,1995;31(Suppl):S320) [5] Yin W M, Guo J T, Wang S H, Li H, Lai W H, Tan M H. Acta Metall Sin, 1995; 31(Suppl): S312(殷为民,郭建亭,王淑荷,李 辉,赖万慧,谭明晖.金属学报,1995;31(Suppl):S312) [6] Guo J T, Yuan C, Yang H C, Lupine V, Maldini M. MetallMater Trans A, 2001; 32A: 1003 [7] Guo J T, Liao E B. In: Iman M A, Denale R, HanadaS, Zhong Z, Lee D N eds, Proc of the Third Pacific RimInter Conf on Adv Mater and Proc (PRICM3), Hawaii:TMS, 1998: 2894 [8] Liao E B, Guo J T, Wang S H. Acta Metall Sin, 1998; 34:278(廖鄂斌,郭建亭,王淑菏.金属学报,1998;34:278) [9] Cuo J T, Liao E B, Guan H R, Li G S, Wang Y L. In: Ellyin F, Provan J W eds, Proc the Eighth International Conference on the Mechanical Behavior of Materials (ICM8), Victoria, B C Canada: Fleming Printing Ltd, 1999: 435 [10] Yin W M, Guo J T, Tan M H, Wang S H, Lai W H, Li H. In: Wang F H ed, The 95' Proc of Conf of China Young Scientists, Shenyang, 1995: 87(殷为民,郭建亭;谭明晖,王淑荷,赖万慧,李 辉.见:王福会主编,95’中国青年学者材料科学学术讨论会,材料的腐蚀与防护文集,沈阳,1995:87) [11] Li H, Guo J T, Tan M H, Wang S H, Lai W H, Yin W M. In: Wang F H ed, The 95' Proc of Conf of China Young Scientists, Shenyang, 1995: 92(李 辉,郭建亭,谭明晖,王淑荷,赖万慧,殷为民.见:王福会主编,95’中国青年学者材料科学学术讨论会,材料的腐蚀与防护文集,沈阳,1995:92) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|