金属间化合物NiAl-Cr(Mo,Hf)合金的研究 |
郭建亭 崔传勇 周兰章 李谷松 |
中国科学院金属研究所;沈阳110016 |
|
引用本文:
郭建亭; 崔传勇; 周兰章; 李谷松 . 金属间化合物NiAl-Cr(Mo,Hf)合金的研究[J]. 金属学报, 2002, 38(11): 1157-1162 .
[1] Noebe R D, Bowman R R, Nathal M V. Inter Mater Rev,1993; 38(4): 193 [2] Cline H E, Walter J L, Lifshin E, Russell R R. MetallTrans, 1971; 2: 189 [3] Cline H E, Walter J L. Metall Trans, 1970; 1: 2907 [4] Johnson D R, Chen X F, Oliver B F, Noebe R D, Whit-tenberger J D. Intermetallic, 1995; 3(1): 99 [5] Darolia R. JOM, 1991; 43(3): 44 [6] Darolia R, Walston W S. In: Nathal M V, Darolia R, LiuC T, Martin P L, Miracle D B, Wagner R, Yamaguchi M eds, Structural Intermetallics 1997, The Minerals, Metals & Materials Society, Pennsyvania, 1997: 585 [7] Editorial Committee of Chinese Aeronautical Material Handbook. Chinese Aeronautical Material Handbook. Beijing: Chinese Standard Press, 1989: 815(中国航空材料手册编辑委员会.中国航空材料手册.北京:中国标准出版社,1989:815) [8] Guo J T, Cui C Y, Chen Y X, Li D X, Ye H Q. Intermetallics, 2001; 9: 287 [9] Cui C Y, Chen Y X, Guo J T, Qi Y H, Ye H Q. MaterSci Eng, 2002; A325(l-2): 187 [10] Cui C Y, Guo J T, Qi Y H, Ye H Q. Scr Mater, 2001; 44:2437 [11] Xing Z P, Guo J T, Han Y F, Yu L G. Metall Mater Trans,1997; 28: 1079 [12] Mukherjee A K, Bird J E, Dorn J E. Trans ASM, 1969;62: 155 [13] Whittenberger J D, Noebe R D, Johnson D R, Oliver BF. Intermetallics, 1997; 5: 173 [14] Coble R L. J Appl Phys, 1963; 34: 1679 [15] Mohamed F A, Langdon T G. Ada Metall Mater, 1974;22: 779 [16] Weetman J. J Appl Phys, 1957; 28: 362 [17] Robinson S L, Sherby O D. Acta Metall Mater, 1976; 24:399 [18] Gonzalez-Doncel G, Sherby O D. Acta Mater, 1993; 41:2792 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|