| 工业灰铸铁凝固组织形成过程的数值模拟 |
| 张云鹏 苏俊义 |
| 西安理工大学铸铁研究所; 西安 710048 |
|
引用本文:
张云鹏; 苏俊义 . 工业灰铸铁凝固组织形成过程的数值模拟[J]. 金属学报, 2000, 36(7): 761-764 .
[1] Minkoff I. Foundryman, 1993; 86(1,2): 16 [2] Kanetkar C S, Stefanescu D M. AFS Trans, 1988; 96: 591 [3] Fras E, Kapturkiewicz W, Lopez H F. AFS Trans, 1992;100: 583 [4] Rappaz M. Int Mater Rev, 1989; 34(3): 93 [5] Goettsch D D, Dantzig J A. Metall Mater Trans, 1994;25A: 1063 [6] Wang Y Q, Lu Y L. Ductile Iron, 1985; (2): 5(王贻青,吕一力,铁球,1985(2):5) [7] Clyne T, Kurz W. Metall Trans, 1981; 12A: 965 [8] Brody H D, Flemings M C. Trans AIME, 1966; 236: 615 [9] Oldfield W A. ASM Trans Q, 1966; 59: 945 [10] Stefanescu D M, Kanetkar C S. AFS Trans, 1987; 95: 139 [11] Magnin P, Kurz W. Acta Metall, 1987; 35: 1119 [12] Jones H, Kurz W. Metall Trans, 1980, 11A: 1265 [13] Stefanescu D M, Upadhya G, Bandyopadhyay D. MetallTrans, 1990; 21A: 997 [14] Johnson W A, Mehl R F. Trans AIME, 1939; 135: 416M |
|