高能球磨对复相A3l3Ti基金属间合金组织和性能的影响 |
傅云义 张津徐 |
上海交通大学材料科学系; 上海 200030 |
|
引用本文:
傅云义; 张津徐 . 高能球磨对复相A3l3Ti基金属间合金组织和性能的影响[J]. 金属学报, 2000, 36(6): 561-566 .
[1] Yamapuchi M, Umakoshi Y, Yamane T Philos Mag 198755A:301 [2]Morris D G,Lerf R Philos Mag,1991 63A:1195 [3] Brown S A Kumar K S J Mate, Res, 1993 8: 1763 [4] Lee KY,Ahn J H Mater,Sic Eng 1997;229A:63 [5]Schneibel J H,Horton J A,Porter W D.Mate,Sci;1992152A:126 [6] Hu G x,Sun J Weng X J h Horton J A,BakerI, Hanada S, Nobe R D、 Schwartz D S eds、 HighTemperature Ordered Intermetallic Alloys VI, Pittsburgh:Matedk Research Society,1995:1083 [7] Fu Y Y, Hu G X Yang W Y, Sun Z Q Acta Metall Sin,1999 35:600(傅云义,胡康祥,杨王现孙祖庆金属学报,19992;35:600) [8] Fu Y Y.Ph D Dissertation, Shanghai Jiaotong University,1998(博云又,上海交通大学博士学位论文,1998). |
|