| 微量元素在Ni基合金凝固过程中分配行为的模拟 |
| 周刚 王文皓 |
| 中国科学院金属研究所; 沈阳 110015 |
|
引用本文:
周刚; 王文皓 . 微量元素在Ni基合金凝固过程中分配行为的模拟[J]. 金属学报, 2000, 36(5): 472-476 .
[1] Woodyatt L R, Sims C T. Trans AIME, 1966; 236: 519 [2] Gessinger G H, Bomford M J. Int Met Rev, 1974; 19: 51 [3] Goulette M J. In: Kissinger R D, Deye D J eds, Sapeml-loys 1996, TMS Pittsburg, PA, 1996. 3 [4] Furr D. Adv Mater Proc, 1999; 3: 33 [5] Zhu Y X, Zhang S N, Xu L Y, Bi J, Hu Z Q, Shi C X.In: Superalloys ed, Saperalloys 1988, Proc of the Fifth IntSamp, Seven Springs, TMS, PA, 1988: 703 [6] Zhu Y X, Zhang S N, Zhang T X, Zhang J H, Hu Z Q, XieX S, Shi C X. In: Antolovich S D, Stusrud R W, MackeyR A eds, Saperalloys 1992, Proc of the Sixth Int Symp,Seven Springs, TMS, PA, 1992: 145 [7] Cao W D, Kennedy R L. In: Loria E A ed, Saperalloys718, 625, 706 and Various Derivatives, TMS Warrendale,PA, 1997: 511 [8] Holt R T, Wallace W. Int Met Rev, 1976; 21: 1 [9] Tamura M, In: Tien J K, Canlfield T eds,Saper-alloys, Sapereomposites and Sapereeramics, AcademicPress, Boston, 1989: 215 [10] Sung J K, Was G S. Corrosion, 1991; 47. 824 [11] Hu Z Q, Sun W R, Guo S R. Acta Metall Sin (EnglishLett), 1996; 9: 443 [12] Horton J A, McKamey C G, Miller M K, Cao W D,Kennedy R L. In: Loria E A ed, Superalloys 718, 625,706 and Various Derivatives, TMS Warrendale, PA, 1997:401 [13] McKamey C G, Garmichael C A, Cao W D, Kennedy RL. Scr Mater, 1998; 38: 485 [14] Laxmanan V. Acta Metall, 1985, 33: 1037 [15] Battle T P, Pehlke R D. Metall Trans, 1990; B21: 357 [16] Zhou G. Ph D Thesis, Institute of Metal Research, TheChinese Academy of Sciences, 1999: 36(周 刚.中国科学院金属研究所博士学位论文,1999:36) [17] Yu J Q, Yi W Z, Chen B D, Chen H J. The Phase Di-agram of Binary Alloy. Shanghai: Shanghai Science andTechnology Press, 1987: 249 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|