| 格子气自动机法模拟冶金多孔介质传输现象 |
| 郑忠 高小强 |
| 重庆大学材料科学与工程学院; 重庆 400044 |
|
引用本文:
郑忠; 高小强 . 格子气自动机法模拟冶金多孔介质传输现象[J]. 金属学报, 2000, 36(4): 433-437 .
[1] Rothman D H, Zaleski S. Red Mod Phys, 1994; 66: 1417 [2] Rothman D H. Geophysics, 1988; 53: 509 [3] Chen S, Diemer K, Doolen G D, Eggert K, Fu C, GutmanS, Thavis B J. Physica, 1991; 47D(1-2): 72 [4] Kohring G A. Physica, 1992; 186A(1/2): 97 [5] Qian Y H, d'Humieres D, Lallemand P. Europhys Lett,1992; 17: 479 [6] Chen H, Chen S, Matthaeus W. Phes Rev, 1992; 45A:5339 [7] Mandelbrot B B. The beetal Geometry of Nature. SanFrancisco: Freeman, 1983: 306 [8] Xie H P. Adv Mech, 1993; 23: 145(谢和平.力学进展,1993;23:145) [9] Szekely J. Translated by Peng Y C, Xu K D, Fan Y Y.Fluid Flow Phenomena in Metals Processing. Beijing:Metallurgical Industry Press, 1985: 270(Szekely J 著.彭一川,徐匡迪,樊养颐译.冶金中的流体流动现象.北京:冶金工业出版社,1985:270) [10] Qin M S, Yang T J. The Analysis cud Modeling of Ironmaking Process Beijing: Metallurgical Industry Press,1991: 49(秦民生,杨天钧.炼铁过程的解析与模拟.北京:冶金工业出版社,1991:49) [11] Wang Z F, Yang T J, Ni X Z. Iron Steel, 1993; 28(8): 1(汪政富,杨天钧,倪学梓.钢铁,1993;28(8):1) [12] Lin R T. Introduce to Heat and Mass Transfer in PorousMedia. Beijing: Science Press, 1995: 39(林瑞泰.多孔介质传热传质引论.北京:科学出版社,1995:39) [13] Wolfram S. Red Mod Phys, 1983; 55: 601 [14] Hardy J, Pomeau Y, de Pazzis O. J Math Phys, 1973; 14:1746 [15] Frisch U, Hasslacher B, Pomeau Y. Phys Red Lett, 1986;56: 1505 [16] d'Humieres D, Lallemand P. Complex Syst, 1987; 1: 599 [17] Hu S X. Chin J Comput Phys, 1989; 6: 457(胡守信.计算物理,1989;6:457) [18] Li Y X, Kang L S, Chen Y P. Lattice Gas Automata. Beijing: Tsinghua University Press, 1994: 50, 68, 149, 154(李元香,康立山,陈毓屏.格子气自动机.北京:清华大学出版社,1994:50,68,149,154) [19] Chen S, Lee M, Zhao K H, Doolen G D. Physica, 1989;37D(1-3): 42 [20] Chen S, Chen H, Doolen G D, Gutman S, Lee M. J StatePhys, 1991; 162: 1121 [21] Zheng Z,Gan X Q, Shi W Y, Xu C S. J Chongqing Univ,1999; 22(3): 117(郑忠,高小强,石万元,徐楚韶.重庆大学学报,1999;22(3):117) [22] Gao X Q, Zheng Z. Chin Sci Abstr 1999; 5: 1507(高小强,郑忠.中国学术期刊文摘(科技快报),1999;5:1507) [23] d'Humieres D, Lallemand P, Frisch U. Europhys Lett,1986; 2: 291 [24] Nasilowski R. J State Phys, 1991; 65(1/2): 97 [25] Vogeler A, Wolf-Gladrow D A. J State Phys, 1993;71(1/2): 163 [26] Kadanoff L P, McNamara G R, Zanetti G. Complex Syst,1987; 1: 791 [27] Weisbuch G. Translated by Ryckebusch S. Complex Systems Dynamica: An Introduction to Automate Network.Redwood: Addison-Wesley Publishing Company, 1991:43 [28] Chen S Y, Chen Y S. Sci Chin, 1990; 20A: 395(陈十一,陈耀松.中国科学,1990;20A:395) [29] Clavin P, Lallemand P, Pomeau Y. J Fluid Mech, 1988;188: 437 [30] Rothman D H, Keller J M. i State Phys, 1988; 52: 1119 [31] Somers J A, Rem P C. Phgsica, 1991; 47D: 39 [32] Li Y X, Kan L S. Neurol Parallel Scientific Comput,1993;1: 43 [33] Yan G W, Hu S X, Shi W P. Chin J Comput Phys, 1997;14: 63(阎广武,胡守信,施卫平.计算物理,1997;14;63) [34] Zheng Z. PhD Thesis, Chongqing University, 1999(郑忠.重庆大学博士学位论文,1999) [35] Yang S W, Hu F. World Sci, 1990; (11): 8(杨硕文,胡非.世界科学,1990;(11):8) [36] Brosa U, Kuttner C, Werner U. J State Phys, 1990; 60:875 [37] Zheng Z, Gao X Q, Shi W Y. Iron Steel, 1999; 34(10): 1(郑忠,高小强,石万元.钢铁,1999;34(10):1) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|