| 高温热应变测试技术及其在耐火浇料上的应用 |
| 王绪东 薛乃彦 |
| 建筑研究总院炉窑工程部; 北京 100088 |
|
引用本文:
王绪东; 薛乃彦 . 高温热应变测试技术及其在耐火浇料上的应用[J]. 金属学报, 2000, 36(4): 438-440 .
[1] Sweeney J, Cross M. J Br Ceram Soc, 1982; 81: 47 [2] Wang J X, Li M Q, Dai L D, Xu Y Q. In: Zhong X C,Wang J X, Li M Q, Dai L D, Xu Y Q eds., The ThirdInternational Symposium on Refractories, Beijing: TheChinese Society for Metals and The Chinese Ceramic Society, 1998: 283 [3] Wang J X, Li M Q, Dai L D, Xu Y Q. In: Zhong X C,Wang J X, Li M Q, Dai L D, Xu Y Q eds., The ThirdInternational Symposium on Refractories, Beijing: TheChinese Society for Metals and The Chinese Ceramic Society, 1998: 161 [4] Zhang B G. Metall Construct Informat, 1984; (4)1: 4(张炳根.冶金建筑情报,1984;(4):1) [5] White J. Refractories J, 1976; 6: 10 [6] Ma L C. Strain Masurement and Season Technology. Beijing: China Metric Publishing, 1993: 261(马良埕.应变电测与传感技术.北京:中国计量出版社,1993:261) |
|