Pb, Zn和Al在熔点附近的导热系数测试 |
蒋绍坚 周孑民 |
中南工业大学应用物理与热能工程系; 长沙410083 |
|
引用本文:
蒋绍坚; 周孑民 . Pb, Zn和Al在熔点附近的导热系数测试[J]. 金属学报, 2000, 36(3): 334-336 .
[1] Zhou J M, Lamvik M. High Temp-High Press. 1998; 30:307 [2] Lamvik M, Zhou J M. Int J Thermophysics, 1995; 16: 567 [3] Metallurgy Furnace Division of Central South Institute ofMining and Metallurgy. Design and Calculation of Nonferrous Metallurgy Furnace, Interior Document, 1973: 38 (中南矿冶学院冶金炉教研室编.有色冶金炉设计及计算.内部资料,1973:38) [4] Peng Q R. A Handbook for Extractive Metallurpy of Nondrrous Metals, Vol.3, The Handbook for Zinc, Cadmium, Leadand Bismuth. Beijing: Metallurgy Industry Press, 1992: 3 (彭秋容.有色金属提取冶金手册第3卷,锌镉铅铋手册.北京:冶金工业出版社,1992:3) [5] American Society for Metals.Translated by Fan Y D. MetalsHandbook, Vol.2, Properties and Selection, Nonferrous Al loys and Pure Metals. Beijing: Mechanical Industry Presss,1994. 907 (美国金属学会编.范玉殿等译,金属手册,第2卷,性能与选择,有色金属与纯金属.北京:机械工业出版社,1994:907) [6] Li C G. Thesis of Master,s Degree, Central South Universityof Technology, 1999 (李长庚.硕士学位论文,中南工业大学,1999) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|