直流磁场作用下Al-18Si合金的凝固行为 |
王艳 边秀房 |
山东工业大学材料科学与工程学院; 济南 250061 |
|
引用本文:
王艳; 边秀房 . 直流磁场作用下Al-18Si合金的凝固行为[J]. 金属学报, 2000, 36(2): 159-161 .
[1] Wang Q D, Jin J Z. Foundry, 1996; (4): 8(王渠东,金俊泽.铸造,1996.2(4):8) [2] Wang Q D, Jin J Z. Trans Nonferrous Met Soc China, 1999;7(1): 125 [3] Wang Q D, Ding W J, Jin J Z. Acta Mater Comp Sin, 1998;15(3): 7(王渠东,丁文江,金俊泽.复合材料学报,1998;15(3):7) [4] Lee H C, Evans J W, Vives C. Metall Trans, 1984; B15: 734 [5] Asai S. ISIJ Int, 1989; 29: 981 [6] Jin J Z, Cao Z Q, Zhou X S, Zhang S R. Acta Metall Sin,1995; 31: 374(金俊泽,曹志强,郑贤淑,张尚儒.金属学报,1995;31:374) [7] Alireza R J, Miwa K, Nishio T. Metall Mater Trans, 1998;A29: 1477 [8] Zhu S L. Atomic Physics. Beijing: The People's Press, 1979:174(褚圣麟.原子物理学.北京:人民出版社,1979:174) |
|