| 钛合金(Ti-17)的动态力学性能和损伤特性 |
| 李强 沈乐天 徐永波 白以龙 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室; 沈阳 110015 |
|
引用本文:
李强; 沈乐天; 徐永波; 白以龙 . 钛合金(Ti-17)的动态力学性能和损伤特性[J]. 金属学报, 1999, 35(5): 491-494 .
[1] Ni J G, Tao C H, Li S N. A course on Damage Mechanics.Beijing: Science Press, 1997: 1(倪金刚,陶春虎,李松年.损伤力学教程.北京:科学出版社,1997. 1) [2] Needleman A. Appl Mech Rev, 1992; 45(3): 53 [3] Bet Y L. Res Mech, 1990; 31: 133 [4] Timothy S P, Hutchings I M. Acta Metall, 1985; 33: 667 [5] Timothy S P. Acta Metall, 1987; 35: 301 [6] Nakkalil R. Acta Metall, 1991; 39: 2553 [7] Xu Y B, Bat Y L. Acta Metall Sin, 1995; 31: A487(徐永波,白以龙.金属学报,1995; 31: A487) [8] Hines J A, Vecchio K S, Ahzi S. Metatl Mater Trans, 1998;29A: 191 [9] Chichili D R, Ramesh K T Hemker K J. Acta Mated 1998;46: 1025 [10] Blazynski T Z. MaterialS at High Strum Rates. London andNew YOrk: Elsevier Applied Science, 1987:133 [11] Hu S S, Wang L L. Vib Impact, 1986; 5: 40(胡时胜,王礼立.振动与冲击,1986;5:40) [12] Li Qiang. The Report of Post-Doctoml Research Work,Shenyang: Institute of Metal Research, The ChineseAcademy of Sciences, 1999(李强.博士后研究工作报告,沈阳:中国科学院金属研究所,1999)9 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|