| Ni-Al系中γ,γ’,β相平衡的实验与热力学分析 |
| 贾成厂 石田清仁 |
| 北京科技大学材料科学与工程学院;北京 100083 |
|
引用本文:
贾成厂; 石田清仁 . Ni-Al系中γ,γ’,β相平衡的实验与热力学分析[J]. 金属学报, 1999, 35(2): 193-197 .
[1] Kaufman L, Nesor H. Met trans, 1975; 5: 1617 [2] Sigli C, SAnchez J M. Acta Met, 1985; 33: 1097 [3] Enomoto M, Harada H. MetallTrans A, 1989; 20A: 643 [4] Inden G, Pitsch W. Z Metallk, 1971; 62: 627, 1972; 63: 253 [5] Schlatte G, Inden G, Pitsch W. Z Metallk, 1974, 65: 94 [6] Nishizawa T, Hao S M, Hasebe M. Acta Metall, 1983; 31:1403 [7] Kikuchi R. Acta Metall, 1977; 25: 795 [8] Tarlor A, Doyle N J. J Appl Cryst, 1972; 5: 201 [9] Georgopoulos P, Cohen J B. Scr Metall, 1977; 11: 147 [10] Taylor A, Floyd R W. J Inst Met, 1952-1953; 81: 25 [11] Hansen M, Anderko K. Constitution of Binary Alloys. NewYork: McGraw full Inc, 1958: 1 [12] Williams R O. Trans AIME, 1959; 215: 1026 [13] Hornbogen E, Kreye H. Z Metallk, 1966; 57: 122 [14] Rastogi K, A J Acta Metall, 1969; 17: 595 [15] Gentry W O, Fine M E. Acta Metall, 1972; 20: 181 [16] Janssen M M P. Metail Trans, 1973; 4: 1623 [17] Sanchez J M, Barefoot J R, Jarrett R N. Acta Metall, 1984;32: 1519 [18] Bradley A J. J Iron Steel Inst, 1949; 163: 19 [19] Nash P, West D R F. Met Sci, 1983; 17: 99 [20] Robertson I M, Wayman C M. Metallogr, 1984; 17: 43 [21] Hilpert K, Kobertz D, Venugopal V. Z Naturforsch, 1987;42A: 1327 [22] Bremer F J. J Cryst Growth, 1988; 87: 185 [23] Ansara I, Sundman B, Willemin P. Acta Metall, 1988; 38:977 [24] Vachet F, Desre P, Bonniier E. C R Acad Sci Paris, 1965,260: 453 [25] Sandakov V M, Esin Yu D, Geld P V. Zh Fiz Khim, 1971;45: 1798 [26] Hultgen R. Selected Values of the Thermodynamic Proper-ties of Binary Alloys. New York : John Wiley and Soos,1973: 1 [27] Pasturel A, Hicter P. Scr Metall, 1983; 17: 841 [28] Colinet C, Bessoud A, Pasturel A. Z Metallk, 1986; 77: 798 [29] Steiner A, Komarek K L. Trans AIME, 1964; 230: 788 [30] Oforka N C, Argent B B. J Less-Common Met, 1985; 114:97 [31] Kaufman L, Hesor H, CALPHAD, 1978; 2: 325 [32] Murray J. Int Met Rev, 1985; 30: 211 [33] Cahn R W, Siemes P A, Geiger J E. Acta Metall, 1987; 35.2737 [34] Tissot P, Dallenbach R. Termo Acta, 1978; 25(2): 143 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|