| 灰铸铁电渣重熔过程石墨球化现象的研究 |
| 储少军;刘海洪;张合义 |
| 北京科技大学冶金学院;北京;100083;北京科技大学冶金学院;北京;100083;北京科技大学冶金学院;北京;100083 |
|
| GRAPHITE NODULAR PHENOMENA DURING THE ESR OF CAST IRON |
| CHU Shaojun; LIU Haihong; ZHANG Heyi (Metallurgical Engineering College;University of Science and Technology Beijing; Beijing 100083)Correspondent: CHU Shaojun; associate professor; Tel: (010)62332790; Fax: (010)62522845 |
引用本文:
储少军;刘海洪;张合义. 灰铸铁电渣重熔过程石墨球化现象的研究[J]. 金属学报, 1998, 34(9): 971-976.
,
,
.
GRAPHITE NODULAR PHENOMENA DURING THE ESR OF CAST IRON[J]. Acta Metall Sin, 1998, 34(9): 971-976.
11981; 548(Paton E O. Electroslag Metall, Kuev: Science Press, 1981: 548 21983;(4):39(Zhychenko B B,Peschanskij I P. Foundry Production, 1983;(4):39) 31986;(3):51(Grachev B A, Gorelov N A, PavlenkoN S. Iron Steel Metall1986;(3): 51) 4 Chu Shaojun, Liu Haihong. Proceeding on 9th ICVM, San Diego, California, 1988; 621 5储少军.首届全国青年冶金学术会议文集,冶金工业出版社,1990:121(Chu S J.Proceedings of the First National Youth Symposium on Metallurgy, Beijing: Metallurgical industry press, 1990; 121) 6储少军.化工冶金,1989;(1):15(Chu S J.Eng Chem Metall, 1989;(1):15) 7 Kishna Murthy G G, HashamA, Pal U B. Ironmaking Steelmaking,1993; 20: 191 8Speelman J L, Caley W F, Leewis K G. Metall Trans, 1989; 20B:31 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|