| Ti对Zr—Mn—V—Ni系合金的微结构和电化学性能的影响 |
| 宋雪雁;雷永泉;张孝彬;张泽;陈立新;杨晓光;吕光烈;张文魁;王启东 |
| 浙江大学材料系;杭州;310027;中国科学院凝聚态物理中心北京电子显微镜实验室;北京;100080;浙江大学材料系;杭州;310027;浙江大学材料系;杭州;310027;中国科学院凝聚态物理中心北京电子显微镜实验室;北京;100080;浙江大学材料系;杭州;310027;浙江大学材料系;杭州;310027;杭州大学中心实验室;杭州310028;浙江大学材料系;杭州310027;浙江大学材料系;杭州310027 |
|
| EFFECT OF Ti ON THE MICROSTRUCTURE AND ELECTROCHEMICAL PROPERTIES OF Zr-Mn-V-Ni ALLOYS |
| SONG Xueyan; LEI Yongquan; ZHANG Xiaobin; ZHANG Ze; CHEN Lixin; YANG Xiaoguang; LU Guanglie; ZHANG Wenkui; WANG Qidong (Department of Materials Science and Engineering; Zhejiang University ; Hangzhou; 310027)(Beijing Laboratory of Electron Microscopy; Center for Condensed Matter Physics; The Chinese Academy of Sciences; P. O. Box 2724; Beijing 100080)(Centeral Laboratory of Hangzhou University; Hangzhou 310028)Correspondent: SONG Xueyan; Tel. (0571) 7951406; Fax: (0571)7951152;E-mail: msecheny@dial. zju. edu. cn |
引用本文:
宋雪雁;雷永泉;张孝彬;张泽;陈立新;杨晓光;吕光烈;张文魁;王启东. Ti对Zr—Mn—V—Ni系合金的微结构和电化学性能的影响[J]. 金属学报, 1998, 34(9): 977-982.
,
,
,
,
,
,
,
,
.
EFFECT OF Ti ON THE MICROSTRUCTURE AND ELECTROCHEMICAL PROPERTIES OF Zr-Mn-V-Ni ALLOYS[J]. Acta Metall Sin, 1998, 34(9): 977-982.
1Ovshinsky S R, Fetcenko M A. J Ross Sci, 1993; 260: 176 2 Huot J, Akiba E, Ogura T, Ishido Y. J Alloys ComP, 1995; 218: 101 3 Hout J, Akiba E, Ishido Y. J Alloys Comp, 1995; 231: 85 4 Joubert J M, Latroche M, Percheron-Guegan A, Bovet J. J Alloys Comp, 1996; 240: 219 5 Yoshida M, Akiba E. J Alloys Comp, 1995; 224: 121 6 Ronnerbr E, Noreus D, Sakai T, Tsukahara M. J Alloys Comp, 1995; 231: 90 7 Miyazaki S, Wayman C M. Acta Metall, 1988; 36. 181 8 Wu S K, Wayman C M. Acta Metall, 1989; 10: 2805 9 Nishida M, Wayman C M, Honma T. Metall fons, 1986; 17A: 1505 10 van Rijswick M H J. In: Andersen A F, Maeland A J eds., Proc Int Symp on the Hydride for Energy Storage,Geilo 1977, Oxford: Pergamon Press, 1978: 261 11 Mccormock M, Badding M E, Vyas B, Iaharak S M, Murphy D W. J Electrochem Soc, 1996; 143: 131 12 Wakao S, Sawa H, Nakano H, Chubachi S, Abe M. J Less-common Met, 1987; 131: 311 |
|