| 金刚石膜与硬质合金基体间的界面状态 |
| 匡同春;刘正义;代明江;周克崧;王德政 |
| 华南理工大学机电系;广州;510641;广东工业大学实验研究中心;广州;510090;华南理工大学机电系;广州;510641;广州有色金属研究院;广州;510651;广州有色金属研究院;广州;510651;广州有色金属研究院;广州;510651 |
|
| STUDY ON THE INTERMCIAL MORPHOLOGY AND STRUCTURE OF DIAMOND THIN FILM-CEMENTED CARBIDE SUBSTRATE |
| KUANG Tongchun; LIU Zhengyi(Department of Mechanical and Electric Engineering; South China University of Technology; Guangzhou 510641)DAI Mingjiang; ZHOU Kesong; WANG Dezheng(Guangzhou Research Institute of Non-Ferrous Metals; Guangzhou 510651) |
引用本文:
匡同春;刘正义;代明江;周克崧;王德政. 金刚石膜与硬质合金基体间的界面状态[J]. 金属学报, 1998, 34(7): 779-784.
,
,
,
,
.
STUDY ON THE INTERMCIAL MORPHOLOGY AND STRUCTURE OF DIAMOND THIN FILM-CEMENTED CARBIDE SUBSTRATE[J]. Acta Metall Sin, 1998, 34(7): 779-784.
1 吕反修.物理,1995;24:606(Lu Fanxiu. Physics, 1995; 24: 606) 2 顾长志,金曾孙功能材料,1997; 28:232(Gu Changzhi,Jin Zengsun.Funct Mater,1997; 28:232) 3 Vandierendonck K, Quaeyhaegens C,Nesladek M, D'Haen J, Vlekken J, D'Olieslaeger M, Stals L M. SurfCoat Technol, 1995; 74-75:819 4 Karner J, Pedrazzini M, Reineck I,Sjostrand M E, Bergmann E. Mater Sci Eng, 1996; A209: 405 5 匡同春,刘正义,周克崧,代明江,王德政功能材料,1997;28:89(Kuang Tongchun,Liu Zhengyi,Zhou Kesong,Dai Mingjiang,Wang Dezheng.Funct Mater,1997; 28:89) 6 Shibuki K, Sasaki K, Yagi M, Suzuki T, Ikuhaya Y. Surf Coat Technol, 1994; 68/69: 369 7 Zhou Kesong, Wang Dezheng, Wang Jian, Feng Biguang. Trans Nonferrous Met Soc Chin, 1993; 3(3): 88 8 Takatsu S, Saijo K, Yagi M, Shibuki K, Echigoya J. Mater Sci Eng, 1991; A140: 747 9 Skogsmo J, Norden H. Refract Met Hand Mated 1992; 11: 49 |
|