| Ml_(1-x)Ca_x(Ni,Co,Al)_5贮氢合金的电化学性能 |
| 陈卫祥;刘伟;陈昀;潘洪革;陈长聘 |
| 浙江大学材料科学与工程系;杭州;310027;浙江大学材料科学与工程系;杭州;310027;浙江大学材料科学与工程系;杭州;310027;浙江大学材料科学与工程系;杭州;310027;浙江大学材料科学与工程系;杭州;310027 |
|
| ELECTROCHEMICAL PERFORMANCES OF M1_(1-x)Ca_x(Ni,Co,Al)_5 HYDROGEN STORAGE ALLOYS |
| CHEN Weixiang; LIU Wei; CHEN Yun; PAN Hongge; CHEN Changpin(Department of Materials Science and Engineering; Zhejiang University; Haugzhou 310027)Comspondent: CHEN Weixiang ; post-doctor Tel: (0571)7951406; Fan(0571)7951152 |
引用本文:
陈卫祥;刘伟;陈昀;潘洪革;陈长聘. Ml_(1-x)Ca_x(Ni,Co,Al)_5贮氢合金的电化学性能[J]. 金属学报, 1998, 34(6): 640-644.
,
,
,
,
.
ELECTROCHEMICAL PERFORMANCES OF M1_(1-x)Ca_x(Ni,Co,Al)_5 HYDROGEN STORAGE ALLOYS[J]. Acta Metall Sin, 1998, 34(6): 640-644.
1 Van Mal H H.Chem Inorg Tech ,1973;45:80 2 Nahm :KS,Jung W B,Lee W Y.HydrogenEnergy ,1990;16:635 3 Osumi Y, Suzuki H, Kato A, Nakane M, Miyaki A.J Chem Soc Jpn,1978; 11: 1472 4 Shinar J, Shaltiel D, Davidov D, Grayevskey A.J Less—Common Met 1978; 60: 209 5 Wang H X,Chen :CP,Wang C S,Wang Q D.J Alloys Comp ,1996;232:192 6 Li Z P, Suda S. Electrochimica Acta ,1995; 40: 467 7 陈卫作,唐致远.郭鹤桐,陈长聘.金属学报,1998;34:184 (Chen W X,Tang Z Y, Guo H T, Chen C R Acta Metall Sin 1998; 34: 184) 8 Iwakura C, Kajiya Y, Yoneyama H.J Electrochem Soc , 1989;136: 1351 |
|