| 磁铁矿在H_2/Ar气氛中还原产物显微结构与形貌变化的原位观测 |
| 王雅蓉;李继光;赵国军;许力贤;李殷泰 |
| 东北大学材料与冶金学院;沈阳;110006;东北大学材料与冶金学院;沈阳;110006;东北大学资源与土木工程学院;沈阳;110006;东北大学材料与冶金学院;沈阳;110006;东北大学材料与冶金学院;沈阳;110006 |
|
| IN SITU OBSERVATIONS OF MICROSTRUCTURAL AND MORPHOLOGICCAL CHANGES OF THE REDUCTION PRODUCT OF MAGNETITE IN H_2/Ar GAS MIXTURES |
| WANG Yarong; LI Jiguang; ZHAO Guojun; XU Lixian; LI Yintai(School of Materials and Metallurgy; Northeastern University; Shenyang 110006)(School of Sources and Civil Engineering; Northeaster University; Shenyang 110016)Comspondent: LI Yintai; professor ; Tel: (024)3914717 Fax (024)3890559 |
引用本文:
王雅蓉;李继光;赵国军;许力贤;李殷泰. 磁铁矿在H_2/Ar气氛中还原产物显微结构与形貌变化的原位观测[J]. 金属学报, 1998, 34(6): 571-578.
,
,
,
,
.
IN SITU OBSERVATIONS OF MICROSTRUCTURAL AND MORPHOLOGICCAL CHANGES OF THE REDUCTION PRODUCT OF MAGNETITE IN H_2/Ar GAS MIXTURES[J]. Acta Metall Sin, 1998, 34(6): 571-578.
1 Pluschkell W, Yoshikoski H Areh Eisenhuttenw, 1970; 41: 715 2 Yoshikoski H, Tokuda M, Ohtani M.J Jpn Inst Met, 1972; 36: 1093 3 Pluschkell W, Sarma B V S. Arch Eisenduttenw, 1973; 44: 161 4 Rao Y K. Metall Trans,, 1979; 10B: 243 5 Moulahid S EL, Rist A. Metall Trans, 1988; 19B: 787 6 Finnstrom U. Scand j Metalll 1976; 5: 134 7 Rau M F,Rieck D,Evans J W.Metall Trans ,1987;18B:257 8 Mattbew S P,Hayes P C.Metall Trans ,1990;21B:141 9 Matthew S P, Hayes P C. Metall Trans, 1990; 21B: 153 |
|