| 钢液RH精炼中喷粉脱硫的动力学 |
| 魏季和;朱守军;郁能文 |
| 上海大学上海市钢铁冶金重点实验室;上海;200072;上海大学上海市钢铁冶金重点实验室;上海;200072;上海大学上海市钢铁冶金重点实验室;上海;200072 |
|
| KINETICS OF DESULPHURIZATION BY POWDER INJECTION AND BLOWING IN RH REFINING OF MOLTEN STEEL |
| WEI Chiho;ZHU Shoujun; YU Nengwen (Shanghai Enhanced Laboratory of Ferrous Metallurgy; Shanghai University; Shanghai 200072) |
引用本文:
魏季和;朱守军;郁能文. 钢液RH精炼中喷粉脱硫的动力学[J]. 金属学报, 1998, 34(5): 497-505.
,
,
.
KINETICS OF DESULPHURIZATION BY POWDER INJECTION AND BLOWING IN RH REFINING OF MOLTEN STEEL[J]. Acta Metall Sin, 1998, 34(5): 497-505.
1远藤公一.制铁研究,19892 335:20(Endoh K. Sada Tetsu Togisata,1989; 335:20) 2 Endoh K.Nippon Steel Technic Rep,1990;45(4) 3Hatakeyama T,Mizukami Y,Igo K,Oita M.Ircn&Steelmaker,1989;15(7):23 4 Myrayama N,Mizukami Y,Azuma K,Onoyma S,Imais T.Proc 6th International Iron and Steel Congress,Vol.3, Napoya: The Iron and Steel Institute of Japan, 1990 151 5 Hale R J,Merk R,Otterman B A Steelmaking Conf Proc,ISS-AIME,Detroit,MI,1990:69 6上原搏英,水藤正人,高桥清志,有吉政弘,桐原理,加藤嘉英。CAMP-ISIJ,1922 5:1240(Ueharal H.Suito M,Takahashi K,Ariyoshi S,Kirihara T,Kato Y.CAMP-ISIJ,1992; 5:1240) 7冈田泰和,深川信,家田幸治,海老原明彦,池宫洋行,真目薰CAMP—ISIJ, 1992;5:1238(Okada Y, Fukawa M, Yata K, Ebihara A, Ikemiya N, Makoto M CAMP—ISIJt 1992 5: 1238) 8冈田泰和,真屋敬一。铁钢,1994;80(1):T9(Okada Y. Shinya H. Tetsu Hagane, 1994; 80(1): T9) 9川合保治,森克已,三宫好史。铁钢,1975;61(1):29(Kawai Y,Mori K,Sanomiya Y.Tetsu Hagane.1975;61(1):29) 10 Oeters F, Strohmenger P, Pluschkell W Arch Eisenhuttenwes, 1973 44: 727 11溶铁·溶滓物性植便览,溶钢·溶滓部会报告,东京:日本铁钢协会,1971:70(Youtetsu.Youkasu No MonoshoUe Yasukata ,YouHagane.Youkasu Tomokazu TsuguNori,Tokyo:ISIJ,1971:70) 12Tsujino R, Nakashima J, Hirai M, Sawada I. ISIJ Int; 1989: 29(7):589 13Szatkowshi M,Tsai M C.Ironmaking Steelmaking,1991;17(4):65 14 Geiger G H,Poirier D R.Transport Phenomena in Metallurgy,Reading Mass:Addison-Wesley;1973:18 15饭田孝道,上田满,森田普一郎.铁钢,1977;63(4):163(Handa N,Kamita M,Morita H,Tetsu Hagane,1977; 63(4):163) 16 Komai T,Mizukami Y, Proc 7th International Conference on Vacuum Metallurgy,Tokyo:ISIJ,1982:1383 17桐原理,加藤嘉英,田口整司,藤井辙也,上原搏英,大宫茂CAMP—ISIJ,1992; 5:1239(Kirihara T, Kato Y, Taguchi H, Fujii W, Uehara H, Osora S. CAMP-ISIJ, 1992; 5: 1239) |
|