| Y_3(Fe,M0)_(29)金属间化合物的结构特性 |
| 潘洪革;杜红林;陈长聘;韩秀锋;杨伏明 |
| 浙江大学材料科学与工程系;杭州;310027;中国原子能科学研究院;北京;102413;浙江大学材料科学与工程系;杭州;310027;中国科学院物理研究所磁学国家重点实验室;北京;100080;中国科学院物理研究所磁学国家重点实验室;北京;100080 |
|
| STRUCTURAL CHARACTERIZATION OF THE Y_3(Fe, Mo)_(29) INTERMETALLIC COMPOUND |
| PAN Hongge; DU Honglin; CHEN Changpin; HAN Xiufeng; YANG Fuming (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)(Institute of Chinese Atomic Energy; Beijing 102413) |
引用本文:
潘洪革;杜红林;陈长聘;韩秀锋;杨伏明. Y_3(Fe,M0)_(29)金属间化合物的结构特性[J]. 金属学报, 1998, 34(5): 473-482.
,
,
,
,
.
STRUCTURAL CHARACTERIZATION OF THE Y_3(Fe, Mo)_(29) INTERMETALLIC COMPOUND[J]. Acta Metall Sin, 1998, 34(5): 473-482.
1 Collocott S J, Day R K; Dunlop J B, Davis R L Camberra, 1992: 7: 137 2 Saito H, Takahashi M, Wakiyama T J Appl Phys. 1988 64: 5965 3 Katter M, Weeker J, Schultz L J Appl Phys, 1991; 70: 3188 4 Cadogan J M, Li H S, Davis R L, Margarian A, Dunlop J B, Gwan P B J Appl Phys, 1994 75: 7120 5 Ivanova G V, Shcherbakova Y V, Belozerov Y V, Yermolenko A S, Teytel Y I Phys Met Metallogr, 1990; 70:63 6 Fuerst C D, Pinkerton; Herbst J F J Magn Magn Mater, 1994; 129: L115 7 Hu Z, Yelon W B Sokid State Commun,1994; 91(3): 223 8 Kalogirou O, Psycharis V Saettas L, Niarchos D J Magn Magn Mater. 1995; 146: 235 9 Margarian A, Dunolp J B, Collocatt S J, Li H S, Cadogan J M, Davis R L to be published 10 Pan H G, Yang G M, Chen C P, Han X F; Tang N; Wang Q D J Magn Magn Mater, 1996: 163: 221 11 Young R A, Makile P E, von Dreele P B J Appl Cryst; 1977: 10: 262 12 梁敬魁.相图与相结构(下册)北京:科学出版社,1993:769 (Liang Jingkui. Phase Diagram and Phase Structre Beijing: Science Press. 1993: 769) 13 Cadogen J M, Li H S, Margarian A, Dunlop J B. Ryan D H, Collocott S J Davis S L J Appl Phus,1994 76:6138 14 Hu B P.Intrinsic Magnetic Properties of the ThMn12 structure Compounds RE(Fe11 Ti) (RE=Rare Earth),PhD Dissertation, Dublin University, 1990 |
|