| 石墨/镁基复合材料中的残余应变、位错及孪晶 |
| 武凤;朱静 |
| 清华大学材料科学与工程研究院;北京;100084;钢铁研究总院;北京;100081 |
|
| THE RESIDUAL STRAIN, DISLOCATION AND TWIN IN Gr(C)/Mg COMPOSITE |
| WU Feng; ZHU Jing (School of Materials Science and Engineering; Tsinghua University; Beijing 100084)(Central Iron and Steel Research Institute; Beijing 100081) |
引用本文:
武凤;朱静. 石墨/镁基复合材料中的残余应变、位错及孪晶[J]. 金属学报, 1998, 34(5): 449-454.
,
.
THE RESIDUAL STRAIN, DISLOCATION AND TWIN IN Gr(C)/Mg COMPOSITE[J]. Acta Metall Sin, 1998, 34(5): 449-454.
1 Vogelsang M, Arsenault R J, Fisher R M. Metall Trans, 1986; 17A: 379 2 Arsenault R J, Wang L, Feng C R. Acta Metall Mater, 1991; 39. 47 3 Wang L, Arsenault R J. MateT Res Soc Symp Proc, 1991; 2l3. 1063 4 Taya M, Mori T. Acta Metall, 1987, 35. 155 5 Funk W, Blank E. Metall Trans, 1988, 19A: 987 6 Li Q, Megusar J, Masur L J, Cornie J A. Mater Sci Eng, 1989, A117: 199 7 Natt S R, Duva J M. Scr Metall, 1986; 20: 1055 8 Arsenault R J, Shi N. Mater Sci Eng, 1986, 81. 175 9 Wu F, Zhu J. Composite Science and Technology, to be published 10 Patankar S N, Sur Yanarayana C, B1ackketter D, Froes F H. J Mater Sci Lett, 1992; 11: 947 11 Kumar S, Singh R N. Acta Metall Mater, 1995; 43: 2417 12 Ickard S M, Mirac1e D B, Majumdar B S, Kendig K L, Rothenflue L, Coker D. Acta Metall Mater,1995; 43: 3105& |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|