| 定向凝固合金DZ17G的高温低周疲劳性能研究 |
| 廖鄂斌;郭建亭;王淑菏 |
| 中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015 |
|
| LCF BEHMIOUR OF DS ALLOY DZ17G AT HIGH TEMPERATURE |
| LIAO Ebin; GUO Jianting; WANG Shuhe(Institute of Metal Research; The Chinese Academy of Scineces;Shenyang 110015) |
引用本文:
廖鄂斌;郭建亭;王淑菏. 定向凝固合金DZ17G的高温低周疲劳性能研究[J]. 金属学报, 1998, 34(3): 278-282.
,
,
.
LCF BEHMIOUR OF DS ALLOY DZ17G AT HIGH TEMPERATURE[J]. Acta Metall Sin, 1998, 34(3): 278-282.
1Guo J T, Ranucci D, Picco E. Mater Sci Eny, 1983; 58: 127 2Guo J T, Ranucai D, Picco E, Strocchi P M. Int J Fatigue, 1984; 6(2): 95 3Clavel M, Pineau A. Moter Sci Eny, 1982; 55: 157 4Decamps B, Brien V, Morton A J. Scr Metall Maten 1994; 31: 793 5谢济洲.机械工程材料,1986;10(5):33 (Xie Jishou. Mater Mech Eng, 1986; 10(5): 33) 6 Okazaki M, Tabata T, Nohmi S. Metall Trans, 1990; 21A: 2201 7 Leverant G R, Gell M. Trans TMS AIME 1969; 245: 1167 ##F278-279-280-281-282 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|