INTERFACES IN PHASE TRANSFORMATIONS
J.W.Christian FRS(Department of Materials; Oxford University; Parks Road; Oxford OX1 3PH; UK)
引用本文:

J.W.Christian. 相变中的界面(英文)[J]. 金属学报, 1997, 33(2): 150-156.
. INTERFACES IN PHASE TRANSFORMATIONS[J]. Acta Metall Sin, 1997, 33(2): 150-156.

全文: PDF(1249 KB)  
摘要: 讨论了各类相变中的界面分类.重构型相变没有共格界面,相变产物形状也无系统性变化.位移型相变有完全共格或部份共格的界面,有可见的相变产物形状变化.完全共格界面出现在无成分变化的马氏体型相变以及有成分变化的扩散位移型相变中.这二种类型界面的迁移依靠台阶(马氏体相变中称之谓相变位错)的运动完成.部分共格界面也可能出现在马氏体型或较为少见的扩散型相变中.
关键词 : 界面,  马氏体相变,  贝氏体相变    
Abstract:The classification of interfaces in various kinds of phase transformation is discussed.Reconstructive phase transformations have incoherent interfaces and there is no systematic change of shape of the product region. Displacive phase transformations have fully coherent or partly coherent interfaces and are detectable by the change of shape.Fully coherent interfaces include martensitic types in which there is no change of composition and diffusional displacive interfaces in which a change of composition occurs.Both types of interface migrate by the motion of steps or ledges which are also called transformation dislocations in the martensite case. Partly coherent interfaces are also martensitic or diffusional. although examples of the latter type are rare.
Key words: interface    martensitic transformation    bainitic transformation
收稿日期: 1997-02-18     
1 D. Hull, Bull. Inst. Met. 2 (1954) 134.
2 B.A.Bilby and J.W.Christian, The Mechamsm of Phase Transformations in Metals (The Institute of Metals, London, 1956) p. 121.
3 C.Laird and H.I.Aaronson, Acta Metall. 18 (1967) 134.
4 Y.C.Liu and H.I.Aaronson, Acta Metall. 18 (1970) 845.
5 J.M.Howe, H.I.Artonson and R.Gronsky, Acta Metall. 33 (1985) 639.
6 J.W.Christian, Proc. Roy. Soc. London A206 (1951) 51.
7 P. Gaunt and J.W.Christian, Acta Metall. 7 (1959) 529,534.
8 S.Takeuchi and T.Honma, Sci. Rep. Res. Inst. Tohoku Univ. A9 (1957) 492,509.
9 T.Waitz and H.P.Karnthaler, Private communication.
10 C.Hitzenberger and H.P.Karnthaler, Philos. Mag. A64 (1991) 151.
11 T.Waitz and H.P.Karnthaler, Philos. Mag. 1996 in course of publication.
12 H.I.Aaronson and M.G.Hall, Metall. Mater. Trans. 25A (1994) 1797.
13 J.W.Christian, Metall. Mater. Trans. 25A (1994) 1821.
14 R.D.J.Garwood, Inst. Met. 83 (1954) 64.
15 K.Marukawa, 1992: ICOMAT-92, p.821.
16 P.Doig and P.E.J.Flewitt, Met. Sci. l7 (1983) 601.
17 Y.Hamada, M.H.Wu and C.M.Wayman, l992: ICOMAT-92, p.833.
18 Q.H.Li, D.L.Liu and T.Ko, 1992: ICOMAT-92, p.845.
19 T.Ko and S.A.Cottrell, J.Iron Steel Inst. 172 (1952) 307.20 S.A.Cottrell and T.Ko, J.Iron Steel Inst. 173 (1953) 224.
21 H.K.D.H. Bhadeshia, Bainite in Steels (The Institute of Metals, London, 1995).
22 E.Swallow and H.K.D.H.Bhadeshia, In course of publication.
[1] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] 王宗谱, 王卫国, Rohrer Gregory S, 陈松, 洪丽华, 林燕, 冯小铮, 任帅, 周邦新. 不同温度轧制Al-Zn-Mg-Cu合金再结晶后的{111}/{111}近奇异晶界[J]. 金属学报, 2023, 59(7): 947-960.
[3] 王福容, 张永梅, 柏国宁, 郭庆伟, 赵宇宏. Al掺杂Mg/Mg2Sn合金界面的第一性原理计算[J]. 金属学报, 2023, 59(6): 812-820.
[4] 李谦, 孙璇, 罗群, 刘斌, 吴成章, 潘复生. 镁基材料中储氢相及其界面与储氢性能的调控[J]. 金属学报, 2023, 59(3): 349-370.
[5] 夏大海, 计元元, 毛英畅, 邓成满, 祝钰, 胡文彬. 2024铝合金在模拟动态海水/大气界面环境中的局部腐蚀机制[J]. 金属学报, 2023, 59(2): 297-308.
[6] 姜江, 郝世杰, 姜大强, 郭方敏, 任洋, 崔立山. NiTi-Nb原位复合材料的准线性超弹性变形[J]. 金属学报, 2023, 59(11): 1419-1427.
[7] 周小宾, 赵占山, 汪万行, 徐建国, 岳强. 渣-金界面气泡夹带行为数值物理模拟[J]. 金属学报, 2023, 59(11): 1523-1532.
[8] 沈莹莹, 张国兴, 贾清, 王玉敏, 崔玉友, 杨锐. SiCf/TiAl复合材料界面反应及热稳定性[J]. 金属学报, 2022, 58(9): 1150-1158.
[9] 宋庆忠, 潜坤, 舒磊, 陈波, 马颖澈, 刘奎. 镍基高温合金K417G与氧化物耐火材料的界面反应[J]. 金属学报, 2022, 58(7): 868-882.
[10] 郑士建, 闫哲, 孔祥飞, 张瑞丰. 纳米金属层状材料强塑性的界面调控[J]. 金属学报, 2022, 58(6): 709-725.
[11] 丁宗业, 胡侨丹, 卢温泉, 李建国. 基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究[J]. 金属学报, 2022, 58(4): 567-580.
[12] 李伟, 贾兴祺, 金学军. 高强韧QPT工艺的先进钢组织调控和强韧化研究进展[J]. 金属学报, 2022, 58(4): 444-456.
[13] 原家华, 张秋红, 王金亮, 王灵禺, 王晨充, 徐伟. 磁场与晶粒尺寸协同作用对马氏体形核及变体选择的影响[J]. 金属学报, 2022, 58(12): 1570-1580.
[14] 卢磊, 赵怀智. 异质纳米结构金属强化韧化机理研究进展[J]. 金属学报, 2022, 58(11): 1360-1370.
[15] 王硕, 王俊升. Al-Li合金中 δ′/θ′/δ′复合沉淀相结构演化及稳定性的第一性原理探究[J]. 金属学报, 2022, 58(10): 1325-1333.