| 应变速率对近全片层组织γ-TiAl合金韧脆转变温度的影响 |
| 王瑜;林栋梁;刘俊亮;C.C.LAW |
| 上海交通大学;国家教委高温材料及高温测试开放实验室;上海200030;上海交通大学;国家教委高温材料及高温测试开放实验室;上海200030;上海交通大学;国家教委高温材料及高温测试开放实验室;上海200030;MaterialsandMechanicsEngineering;UnitedTechnologiesCompany-Pratt&Whitney400MainStreel;EastHartford;CT06108;U.S.a |
|
| THE EFFECT OF STRAIN RATE ON THE BRITTLE-TO-DUCTILE TRANSITION |
| WANG Yu;LIN Dongliang(T.L.Lin); LIU Junliang(Shanghai Jiao Tong University;High-Temperature Materials and High-Temperature Testing Open Laboratory of Nalional Education Committee of China; Shanghai 200030); C.C.Law (Materials and Mechanics Engineering; United Technologies Company-Pratt & Whitney 400 Main Streel; East Hart ford; CT 06108; U.S.a) |
引用本文:
王瑜;林栋梁;刘俊亮;C.C.LAW. 应变速率对近全片层组织γ-TiAl合金韧脆转变温度的影响[J]. 金属学报, 1997, 33(10): 1021-1027.
,
,
,
.
THE EFFECT OF STRAIN RATE ON THE BRITTLE-TO-DUCTILE TRANSITION[J]. Acta Metall Sin, 1997, 33(10): 1021-1027.
1 Kim Y W, JOM, 1994; 46:30 2 Huang S C,Hall E L.Metall Trans a,1991;22:47 3 Kumpfert J,Kim Y W,Dimiduk D M.Mater Sci Eng a,1995;192/193:465 4 Zener C,Hollomon J J appl Phhs,9144;39:163 5 Kroll S,Mehrer H,Stolwijk N,Herzig C,Rosenkranz R,Frommeyer G.Z Mettallkd,1992;83:591 6 Sprengel W, Oikawa N Nakajima H. Intermetallics.1996; 4: 185 7 Groves G W,Kelly a.Phil Mag,1969;19:977 8 Schafrik R E. Metall Trans a, 1977; 8:1003 9 Kad B K. Fraser H L. Phil Mag,1994; 69:689{ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|