| 金属基复合材料的现状与展望 |
| 吴人洁 |
| 上海交通大学;上海;200030 |
|
| THE PRESENT CONDITION AND PROSPECTS ON METAL MATRIX COMPOSITES |
| WU Renjie (Shanghai Jiaotong University; Shanghai 200030) |
引用本文:
吴人洁. 金属基复合材料的现状与展望[J]. 金属学报, 1997, 33(1): 78-84.
.
THE PRESENT CONDITION AND PROSPECTS ON METAL MATRIX COMPOSITES[J]. Acta Metall Sin, 1997, 33(1): 78-84.
1吴人洁,复合材料学报,1987;41 2 Keily A Composites Sci Technol.1989;23:171 3 Lai S W,Chung D D L J Mater Sci 1994;29:3128 4 A J Cook Mater Sci Eng,1991;A144 5 Yue W,Lavernia E J JOM,1991;8:16 6Helmersson U, el al J Appl Phys,1987 62:481 7 Aronson R B.Machine Design,1985;8 68 8 Marsaden K JMetals 1985 6 59 9 Allison J E,Cole G S.JOM,1993;45:19 10吴人洁,李鹏兴 见:李恒德,肖纪美主编,材料的表面与界面,北京;清华大学出版社,1990 11储双杰,吴人活电子显微学报,1996,待发表 12王浩伟,储双杰,张国定,吴人洁 机械工程学报,1996;31(1):97 13 Wu R J Proceedings of ICCM 6 &ECCM-2 1987;2:128 14 Fulcunaga H,Komatsu S,Kanoh Y Bull Jpn Soc Mech Eng,1983;26;1814 15 Stefanesu D M,Dhindars B K,et al.Metall Trans 1988;19A:2847 16储双杰,金瑞,王浩伟,吴人洁,赵昌正.有色金属,1996 待发表 17储双杰,吴人洁.金属学报,待发表 18Stefanescu D M.Key Eng Mater,1993;79-80:74 19谢国宏.材料工程,1994(12):5 20Clyne T W,Bader M G.Proc of International Conference on Composite Materials TMS-ALME,1985:755 21Doncel G G,Karmarker S D,Divecha A P,Sherby O D Composile Sci Tech 1989; 35:105 22 Schuster D JOM,1993;45:26 23 Newkirk M S Ukgnhart A W.J Mater Res,1986;1:8 24 Denillmnscat T,Robin A L.Metall Trans ,1994 25A:2357 25 Clear T D,Johnson W B. Ceram Eng Sci Proc,1989;10:7 26 崔容翔,吴人洁 金属学报,1996;32 101p |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|