| 加硼HAl77-2铝黄铜的组织和力学性能 |
| 王吉会;姜晓霞;李诗卓 |
| 中国科学院金属研究所 |
|
| ^MICROSTRUCTURE AND MECHANICAL PROPERTIES OF BORON-MODIFIED HAI 77-2 BRASS |
| WANG Jihui;JIANG Hiaoxia;LI Shizhuo(Institute of Metal Research;Chinese Academy of Sciences.Shenyang 110015)(Manuscript received 1994-12-20) |
引用本文:
王吉会;姜晓霞;李诗卓. 加硼HAl77-2铝黄铜的组织和力学性能[J]. 金属学报, 1995, 31(7): 315-319.
,
,
.
^MICROSTRUCTURE AND MECHANICAL PROPERTIES OF BORON-MODIFIED HAI 77-2 BRASS[J]. Acta Metall Sin, 1995, 31(7): 315-319.
| 1青木清,和泉修.日本金属学会志,1979;43:11902郭建亭,孙超,谭明晖,赖万慧.金属学报,1990;26:A203 孙 理,姜晓霞.中国腐蚀与防护学报,1990;10:3714 周业蓉.腐蚀科学与防护技术1989;创刊号:285 窦照英,材料保护,1980;13(6):166 LangeneggerEE、Ronbison,FP.Corrosion,1969;25(3):1377 邱万川,汪的华,邹津耘.全国第五届正电子湮没谱学会议论文集,1993:84 |
|