| 晶体取向对单晶高温合金一次枝晶间距的影响 |
| 何国;李建国;毛协民;傅恒志 |
| 西北工业大学;北京科技大学新金属材料国家重点实验室 |
|
| INFLUENCE OF CRYSTAL ORIENTATION ON THE PRIMARY DENDRITE ARM SPACING OF A SINGLE CRYSTAL SUPERALLOY |
| HE Guo;LI Jianguo;MAO Hiemin;FU Hengzhi(Northwestern Polytechnical University;Hi'an 710072)(Manuscript received 1994-09-13.in revised form 1995-03-13) |
引用本文:
何国;李建国;毛协民;傅恒志. 晶体取向对单晶高温合金一次枝晶间距的影响[J]. 金属学报, 1995, 31(7): 309-314.
,
,
,
.
INFLUENCE OF CRYSTAL ORIENTATION ON THE PRIMARY DENDRITE ARM SPACING OF A SINGLE CRYSTAL SUPERALLOY[J]. Acta Metall Sin, 1995, 31(7): 309-314.
| 1BurdenMH,HuntJD.JCrystGrowth.1974;22;99.1092TrivediR,JCrystGrowth,1980:49:2193KurzW,FisherDJ.ActaMetall,1981;29:114KurzW,FisherDJ.FundamentalsofSolidification.Aedermannsdorf:TransTechPublicationsLtd.1984:805TrivediR,MasonJTMasonJ.MetallTransA,1991:22A:2356TrivediR.SeetharamanV.EshelmanMA.MetallTransA,1991;22A:5857HuangSC,GlicksmanMEActaMetall,1981;29:7178何国.西北工业大学博士学们论文,1994 |
|