| 显微组织对Ti_3Al-Nb系合金疲劳裂纹扩展行为的影响 |
| 艾素华;关少轩;冯泽民;葛景岩 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室;东北大学 |
|
| EFFECT OF MICROSTRUCTURE ON FATIGUE CRACK GROWTH OF Ti_3Al-Nb ALLOYS |
| AI Suhua;GUAN Shaoxuan(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy; of Sciences; Shenyang 110015).FENG Zemin; GE Jingyan(Northeastern University; Shenyang 110006) |
引用本文:
艾素华;关少轩;冯泽民;葛景岩. 显微组织对Ti_3Al-Nb系合金疲劳裂纹扩展行为的影响[J]. 金属学报, 1995, 31(4): 183-190.
,
,
,
.
EFFECT OF MICROSTRUCTURE ON FATIGUE CRACK GROWTH OF Ti_3Al-Nb ALLOYS[J]. Acta Metall Sin, 1995, 31(4): 183-190.
| 1LipsittHA,ShechtmanD,SchafrikR.MetallTrnas,1980;11A:13692YangWJS.JMaterSciLett,1982;1:1993LiuCT,StieglerJOReprintSeries9,ICTH,TriesteItaly,1984;226:6364KhataceA,FlowerHM,WestDRF.JMaterEng,1988;10:375StrychorR,WilliamsJC,SoffaWA.MetallTrans,1988;19A:225 6WittennauerJ,BassiC,Walser B.ScrMetall,1989;23:13817AswathP B,SureshS.MetallTrans,1991:22A:8178RaoKTV,OdetteG R,RichieR O.ActaMetall1992;40:3539张 鹰,李学明,高 扬.材料工程,1992;4:2210ChaveRA,BeeversCJ,BowenP.In:BailonJB,DicksonJIeds.,Fatigue'93,1993;2:100711GaoH,BrownMW,MillerKJ.Fatigue EngMater Struct,1982;5:112ElberW.Eng FracMech,1970,2:3713SureshS.FatigueofMaterialsCambridgeUniversityPress,199114SwainMV,KimNJ.In:KishiT,TakedaN,Kagawa Y eds.,Proc3rdIntSAMPE,Japan,1993:1519 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|