| 两种Ti_3Al在水中的低频疲劳研究 |
| 邢志强;程咏梅;褚武扬 |
| 北京工业大学;北京科技大学 |
|
| LOW-FREQUENCY FATIGUE OF TWO Ti_3Al INTERMETALLICS IN DISTILLED WATER |
| XING Zhiqiang; CHENG Yongmei(Beijing Polytechnic University;100022);CHU Wuyang(University of Science and Technology Beijing; 100083)(Manuscript received 94-03-10;in revised form 94-07-19) |
引用本文:
邢志强;程咏梅;褚武扬. 两种Ti_3Al在水中的低频疲劳研究[J]. 金属学报, 1995, 31(1): 34-39.
,
,
.
LOW-FREQUENCY FATIGUE OF TWO Ti_3Al INTERMETALLICS IN DISTILLED WATER[J]. Acta Metall Sin, 1995, 31(1): 34-39.
| 1FleischerRL,DimidukDM,LipsittHA.AnnuRevMaterSci,1989;19:2312Bavarian,B,HarutouniS,ZamanzadehM.MaterSciEng,1992;A153:6133ChuWY,ThompsonAW,WilliamsJC.ActaMetallMater,1992;40:4554ChuWY,ThompsonAW.MetallTrans,1991;22A:715褚武扬,肖纪美,ThompsonAW.金属学报,1992;28:A676ShihDS,ScarrGK,WasielewskiGE.ScrMetall,1989;23:9737张跃.北京科技大学博士学位论文,19938ManorE,EliezerD.ScrMetall,1989;23:13139 ZhangY,WangYB,ChuWY,HsiaoCM,ThompsonAW.ScrMetallMater,1992;26:92510张跃,王燕斌,褚武扬,肖纪美.中国腐蚀与防护学报,待发表11张跃,王燕斌,褚武扬,肖纪美.中国科学,1994;24A:55112RhodesD,RadonJC.IntJFatigue,1979;15:R6513XingZQ,SongYJ,TuMJ.FatigueEngMaterStruct,1992;15:2314PanasyukVV,RatychLV,DmytrakhIN.FatigueEngMaterStruct,1984;7:115卓向东,林昌健,田昭武.中国腐蚀与防护学报,1985;5:27716HoarTP,JonesRW.CorrosSci,1973;l3:72 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|