| 激光表面熔凝处理ZAlSi12合金的亚结构特征 |
| 梁工英;李成劳;周家瑾 |
| 西安交通大学 |
|
| SUBSTRUCTIONAL FEATURE OF SURFACE LASER MELTED ZAlSi 12 ALLOY |
| LIANG Gongying; LI Chenglao; ZHOU Jiajin(Xi'an Jiaotong University) |
引用本文:
梁工英;李成劳;周家瑾. 激光表面熔凝处理ZAlSi12合金的亚结构特征[J]. 金属学报, 1994, 30(22): 471-475.
,
,
.
SUBSTRUCTIONAL FEATURE OF SURFACE LASER MELTED ZAlSi 12 ALLOY[J]. Acta Metall Sin, 1994, 30(22): 471-475.
| 1FerraroF,NannettiCA,CampelloM,SeninA,In:QuenzerAed.,Proc.3rdInt.ConfonLasersinManufacturing,3-5June,1986,Paris,BedfordUK:IFS(Publications)Ltd,1986:2332LiangGongying,ZhouJiayin,ZhengQiguang.ChineseJournalofLasers,1993;B2:2413KobayashiKF,HoganLM.MaterSci,1985;20:19614ShuzuLU,HellawellA.CrystalGrowth,1985;73:3165魏全金.材料电子显微分析.北京:冶金工业出版社,1990:186 |
|