定向凝固Fe—C共晶合金的组织参数与拉伸特性 |
蒋建清 |
东南大学 |
|
STRUCTURE PARAMETER AND TENSILE PROPERTIES OF UNIDIRECTIONALLY SOLIDIFIED Fe-C EUTECTIC ALLOY |
JIANG Jianqing Southeast University; Nanjing |
引用本文:
蒋建清. 定向凝固Fe—C共晶合金的组织参数与拉伸特性[J]. 金属学报, 1993, 29(9): 35-41.
.
STRUCTURE PARAMETER AND TENSILE PROPERTIES OF UNIDIRECTIONALLY SOLIDIFIED Fe-C EUTECTIC ALLOY[J]. Acta Metall Sin, 1993, 29(9): 35-41.
1 Eilliott A. Eutectic Solidification Processing. London: Butterworths, 1983: 48 2 Kurz W,Fisher D J著;毛协民,包冠乾译.凝固原理.西安:西北工业大学出版社,1987:95 3 胡汉起.金属凝固.北京:冶金工业出版社,1985:215 4 蒋建清.东南大学博士学位论文,1990 5 蒋建清,舒光冀.东南大学学报,1991;(6) :92 6 Jiang Jianqing. In: Yan Dongsheng, Shi Changxu, Li Hengde eds., China--MRS International 1990 Symposium, Vol.Ⅴ, Holland: Elsevier, 1991: 200 7 蒋建清.东南大学学报,1993:(2) :19 |
|