| 金属间化合物Ni_3Al点缺陷的理论计算 |
| 孙坚;林栋梁 |
| 上海交通大学;上海交通大学材料科学系;教授;上海200030 |
|
| THEORETICAL CALCULATION OF POINT DEFECTS IN Ni_3Al |
| SUN Jian;LIN Dongliang Shanghai Jiaotong University professor;Department of Materials Science;Shanghai Jiaotong University; Shanghai 200030 |
引用本文:
孙坚;林栋梁. 金属间化合物Ni_3Al点缺陷的理论计算[J]. 金属学报, 1993, 29(4): 25-29.
,
.
THEORETICAL CALCULATION OF POINT DEFECTS IN Ni_3Al[J]. Acta Metall Sin, 1993, 29(4): 25-29.
1 Dasgupta A, Smedskjar L C, Legnini D G, Siegel R W. Mater Lett, 1985; 3: 457 2 杨文英,吕反修,章守华.金属学报,1990;26A:385 3 孙坚.上海交通大学博士学位论文,1992 4 Foils S M, Daw M S. J Mater Res, 1987; 2: 5 5 Seeger A, Mehrer H. Vacancies and Interstitials in Metals. Amsterdem: North-Holland, 1970; 1 6 Liu C T, White C L, Horton J A. Acta Metall, 1985; 33: 213) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|