| YBa_2Cu_3O_(7-x)-Ag界面与表面的研究 |
| 樊永年;汤宝珍;乔桂文 |
| 中国科学院金属研究所;副研究员沈阳110015;中国科学院金属研究所;中国科学院金属研究所 |
|
| STUDY OF INTERFACES AND SURFACES OF YBa_2Cu_3O_(7-x)-Ag |
| FAN Yongnian; TANG Baozhen; QIAO Guiwen (Institute of Metal Research; Academia Sinica; Shenyang) |
引用本文:
樊永年;汤宝珍;乔桂文. YBa_2Cu_3O_(7-x)-Ag界面与表面的研究[J]. 金属学报, 1992, 28(7): 70-73.
,
,
.
STUDY OF INTERFACES AND SURFACES OF YBa_2Cu_3O_(7-x)-Ag[J]. Acta Metall Sin, 1992, 28(7): 70-73.
1 Mizushima K, Sagoi M, Miura T, Yoshida J. Jpn J Appl Phys, 1988; 27: L1489 2 Salama K, Selvamanickam V, Gao L, Sun K. Appl Phys Lett, 1989; 54: 2352 3 汤宝珍,崔永姬,樊永年,乔桂文.全国高温超导学术会议论文集(一),宝鸡:稀有金属加上研究所出版,1988:19-12 4 Nishio T, Itoh Y. Ogasawara F, Suganuma M, Yamada Y, Mizutani U. J Mater Sci, 1989; 24; 3228 5 Singh J P, Leu H J, Poeppel R B. Van Voorhees E, Goudey G T, Winsley K. Shi D. J Appl Phys, 1989; 66: 3154 6 Mansour A N, Dallek S, Anderson G R. Physics, 1989; B158: 519 |
|