| 溅射NdFeB薄膜合金的磁各向异性 |
| 顾本喜;翟宏如;H.HOMBURG;S.METHFESSEL |
| 南京大学;南京大学;西德波鸿鲁尔大学;西德波鸿鲁尔大学 |
|
| MAGNETIC ANISOTROPY IN SPUTTERED NdFeB FILMS |
| GU Benxi;ZHAI Hongru Nanjing University; HOMBURG H; METHFESSEL S Ruhr-Universitat Bochum; Germany |
引用本文:
顾本喜;翟宏如;H.HOMBURG;S.METHFESSEL. 溅射NdFeB薄膜合金的磁各向异性[J]. 金属学报, 1991, 27(5): 116-119.
,
,
,
.
MAGNETIC ANISOTROPY IN SPUTTERED NdFeB FILMS[J]. Acta Metall Sin, 1991, 27(5): 116-119.
1 Sagawa M, Fujimura S, Togawa N, Yamamoto H, Matsuura Y. J Appl Phys, 1984: 55: 2083 2 Herbst J F, Croat J J, Pinkerton F E, Yelon W B. Phys Rev, 1984; B29: 4176 3 Croat J J, Herbst J F, Lee R W, Pinkerton F E. J Appl Phys, 1984; 55: 2078 4 Gu B X, Shen B G, Methfessel S, Zhai H R. Solid State Commun, 1989; 70: 933 5 Gu B X, Shen B G, Zhai H R. Phys Rev, 1990; B42: 10648 6 Cadieu F J, Cheung T D, Wickramasekara L, Kamprath N. IEEE Trans Magn, 1986; MAG 22: 752 7 Cadieu F J, Cheung T D, Wickramasekara L. J Magn Magn Mater, 1986; 54--57: 535 8 Cadieu F J, Cheung T D, Wickramasekara L, Kamprath N, Hegde H, Liu N C. J Appl Phys, 1987; 62: 3866 9 Zasadzinski J F, Segre C U, Rippert E D. J Appl Phys, 1987; 61: 4278 10 Gu B X, Homburg H, Methfessel S, Zhai H R. Phys Status Solidi, 1990; 120: 159 11 Gu B X, Hsia Y, Liu R, Zhai H R, Homburg H. Methfessel S. Hyperfine Interact, 1990; 55: 957 12 Tenaud P, Chamberod A, Vanoni F. Solid State Commun, 1987; 63: 30 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|