| 定向凝固的界面形态转变 |
| 黄卫东;周尧和 |
| 西北工业大学凝固技术国家重点实验室;讲师西安(710072);西北工业大学凝固技术国家重点实验室 |
|
| INTERFACE MORPHOLOGY TRANSITIONS DURING DIRECTIONAL SOLIDIFICATION IN A TRANSPARENT MODEL ALLOY |
| HUANG Weidong;ZHOU Yaohe National Solidification Processing Laboratory; Northwestern Polytechnical University; Xi'an |
引用本文:
黄卫东;周尧和. 定向凝固的界面形态转变[J]. 金属学报, 1991, 27(2): 8-13.
,
.
INTERFACE MORPHOLOGY TRANSITIONS DURING DIRECTIONAL SOLIDIFICATION IN A TRANSPARENT MODEL ALLOY[J]. Acta Metall Sin, 1991, 27(2): 8-13.
1 Eshelman M A, Trivedi R. Acta Metall, 1987; 35: 2443 2 Tewari S N, Laxmanan V. Metall Trans, 1987; 18A: 167 3 Jackson K A, Hunt J D. Trans AIME, 1966; 236: 1129 4 Schaefer R J, Coriell S R. Metall Trans, 1984; 15A: 2109 5 黄卫东.西北工业大学博士学位论文,1989c |
|