| Mn-Cu合金马氏体相变与沉淀的内耗 |
| 张志方;张志东;袁方;王业宁 |
| 南京大学固体微结构实验室;南京210008;南京大学;沈阳中国科学院金属研究所;南京大学;南京大学 |
|
| INTERNAL FRICTIONS OF MARTENSITIC TRANSFORMATION AND PRECIPITATION IN Mn-Cu ALLOY |
| ZHANG Zhifang;ZHANG Zhidong;YUAN Fang;WANG Yening Loboratory of Solid State Microstructures; Nanjing University |
引用本文:
张志方;张志东;袁方;王业宁. Mn-Cu合金马氏体相变与沉淀的内耗[J]. 金属学报, 1991, 27(1): 7-10.
,
,
,
.
INTERNAL FRICTIONS OF MARTENSITIC TRANSFORMATION AND PRECIPITATION IN Mn-Cu ALLOY[J]. Acta Metall Sin, 1991, 27(1): 7-10.
1 王力田,葛庭燧.金属学报,1988;24:A147 2 谢存毅,文亦汀,朱贤方.金属学报,1988;24:A71 3 Zaaraoui Z, Bouquet G, Dubois B. J Phys (Paris), 1983; 44 (C9) :259 4 Stokes H J, Hewin I D. J Inst Met, 1960--61; 89: 77 5 Numakura H Koiwa M. Trans Jpn Inst Met, 1985; 26: 653 6 Wang Yening, Gu Min, Sun Linhai. J Phys: Condens Matter, 1989; 1(50) : 10039 7 Miner R E, Wilson T L, Jackson J K. TMS AIME, 1969; 245: 1375 8 Cannelli G, Mazzolai F M. Nuovo Cimento, 1969; LXIVB: 171 9 Vitek J M, Warlimont H. Met Sci, 1976; 10: 7 |
|