| 预应变对16MnR钢断裂韧性的影响 |
| 朱汉兴;蒋家羚;李长春;薛继良 |
| 华中理工大学力学系;武汉市430074;浙江大学;华中理工大学;浙江大学 |
|
| EFFECT OF PRESTRAIN ON FRACTURE TOUGHNESS OF 16MnR STEEL |
| ZHU Hanxing;LI Changchun Huazhong University of Science and Technology; Wuhan. JIANG Jialing;XUE Jiliang Zhejiang University; Hangzhou |
引用本文:
朱汉兴;蒋家羚;李长春;薛继良. 预应变对16MnR钢断裂韧性的影响[J]. 金属学报, 1991, 27(1): 49-54.
,
,
,
.
EFFECT OF PRESTRAIN ON FRACTURE TOUGHNESS OF 16MnR STEEL[J]. Acta Metall Sin, 1991, 27(1): 49-54.
1 赵志业.金属的塑性变形与轧制理论,北京:冶金工业出版社,1980 2 曹乃光.金属的塑性加工原理,北京;冶金工业出版社,1983 3 肖纪美.合金相与相变,北京:冶金工业出版社,1987 4 Amouzouvi K F, Bassim M N. Mater Sci Eng. 1983; 60: 1 5 Amouzouvi K F, Bassim M N. In: Simpson L ed, Fracture Problems and Solutions in the Energy Industry, Proc 5th Can. Fracture Conf, September 3--4, 1981, Oxford: Pergamon, 1982: 179< |
|