| 合金在电磁场中凝固时生成的特殊表面 |
| 任忠鸣;苏辉;金俊泽 |
| 大连理工大学铸造工程研究中心;大连理工大学;大连理工大学 |
|
| Si-RICH LAYER FORMATION DURING DIRECTIONAL SOLIDIFICATION OF Al-Si EUTECTIC ALLOY IN ELECTROMAGNETIC FIELD |
| REN Zhongming;SU Hui;JIN Junze Dalian University of Technology |
引用本文:
任忠鸣;苏辉;金俊泽. 合金在电磁场中凝固时生成的特殊表面[J]. 金属学报, 1990, 26(5): 150-152.
,
,
.
Si-RICH LAYER FORMATION DURING DIRECTIONAL SOLIDIFICATION OF Al-Si EUTECTIC ALLOY IN ELECTROMAGNETIC FIELD[J]. Acta Metall Sin, 1990, 26(5): 150-152.
1 Shingu P H, Kurosaki M, Jin-Junze. Trans Jpn Inst Met, 1986; 27: 546 2 Miwa K, Kakamu T, Ohashi T. Trans Jpn Inst Met, 1985; 26: 549 3 桃野正,井川克也.轻金属,1975;25:403x |
|