| 熔渣下金属熔池流动现象的数学模拟 |
| 曲英;杨健;徐保美 |
| 北京科技大学冶金系;教授;北京(100083);北京科技大学;北京科技大学 |
|
| MATHEMATICAL MODELLING OF FLOW PHENOMENA IN METAL BATH COVERED WITH MOLTEN SLAG |
| QU Ying;YANG Jian;XU Baomei University of Science and Technology Beijing Department of Metallurgy;University of Science and Technology Beijing; Beijing 100083 |
引用本文:
曲英;杨健;徐保美. 熔渣下金属熔池流动现象的数学模拟[J]. 金属学报, 1990, 26(3): 85-91.
,
,
.
MATHEMATICAL MODELLING OF FLOW PHENOMENA IN METAL BATH COVERED WITH MOLTEN SLAG[J]. Acta Metall Sin, 1990, 26(3): 85-91.
1 Szekely J. Dilawari A H, Metz R. Metall Trans., B, 1979; 10B: 33 2 Sahai Y, Guthrie R I L. Metall Trans, 1982; 13B: 193, 203 3 Zhang Jia-yun, Du Si-shen, Wei Shou-kun. Ironmaking Steelmaking, 1985; 12 (6) : 249 4 Hsiao Tse-chiang, Lehner T, Kjellberg B. Scand J Metall, 1980; 9: 105 5 Qu Y, Liang Y, Liu L. SCANINJECT III, 1983: article 21 6 王尚槐,薛成志.钢铁,1986;(10) :19 7 彭一川,肖泽强.化工冶金,1988;(1) :71 8 Mazumdar D, Nakajima H, Guthrie R I L. Metall Trans, 1988; 19B: 507 9 Gosman A D, Pun W M, Runchal A K, Spalding D B, Wolfstein M. Heat and Mass Transfer in Recirculating Flows, New York: Academic Press, 1969K |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|