| 矿岩粉碎全过程能耗-粒度关系的连续损伤理论研究 |
| 朱毅;徐小荷 |
| 东北工学院;东北工学院 |
|
| A CONTINUOUS DAMAGE APPROACH TO RELATIONSHIP BETWEEN SIZE REDUCTION AND ENERGY CONSUMPTION DURING ORE COMMINUTION |
| ZHU Yi;XU Xiaohe Northeast University of Technology; Shenyang Department of Mining;Northeast University of Technology;Shenyang 110006 |
引用本文:
朱毅;徐小荷. 矿岩粉碎全过程能耗-粒度关系的连续损伤理论研究[J]. 金属学报, 1990, 26(3): 81-84.
,
.
A CONTINUOUS DAMAGE APPROACH TO RELATIONSHIP BETWEEN SIZE REDUCTION AND ENERGY CONSUMPTION DURING ORE COMMINUTION[J]. Acta Metall Sin, 1990, 26(3): 81-84.
1 Zhu Yi, Xu Xiao-he. J Eng Fract Mech, 1990; 35: 647 2 Kachanov L M. Mech Mater, 1982; 1: 19 3 朱毅,徐小荷.有色金属,1989;41:1 4 Perry J H. Chemical Engineer Handbook, 3rd ed., New York: McGraw-Hill, 1950: 417 5 朱毅.东北工学院博士论文,1988 6 Schuhmann R J. AIME TP 1189, 1940 7 Charles R J. Trans AIME, 1957; 208: 80 |
|