钝化处理对316L不锈钢血液相容性的影响 |
史永娟1,2,任伊宾1,张炳春1,杨柯1 |
1. 中国科学院金属研究所, 沈阳 110016
2. 中国科学院研究生院, 北京 100049 |
|
THE EFFECT OF PASSIVATION ON THE HAEMOCOMPATIBILITY OF 316L STAINLESS STEEL |
SHI Yongjuan 1,2, REN Yibin 1, ZHANG Bingchun 1, YANG Ke 1 |
1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2. Graduate School of Chinese Academy of Sciences, Beijing 100049 |
引用本文:
史永娟 任伊宾 张炳春 杨柯. 钝化处理对316L不锈钢血液相容性的影响[J]. 金属学报, 2011, 47(12): 1575-1580.
,
,
,
.
THE EFFECT OF PASSIVATION ON THE HAEMOCOMPATIBILITY OF 316L STAINLESS STEEL[J]. Acta Metall Sin, 2011, 47(12): 1575-1580.
[1] Shahryari A,Azari F, Vali H, Omanovic S. Acta Biomater, 2010; 6: 695
[2] Shih C C, Shih C M, Su Y Y, Su L H J, Chang M S, Lin S J. Corros Sci, 2004; 46: 427
[3] Shahryari A, Omanovic S, Szpunar J A. Mater Sci Eng, 2008; C28: 94
[4] Barbosa M A. Corros Sci, 1983; 23: 1293
[5] Noh J S, Laycock N J, Gao W, Wells D B. Corros Sci, 2000; 42: 2069
[6] Hong T, Ogushi T, Nagumo M. Corros Sci, 1996; 38: 881
[7] Ma L Y, Ding Y, Ma L Q, Yao C R, Shen W D. Surf Technol, 2007; 36: 39
(马李洋, 丁毅, 马立群, 姚春荣, 沈卫东. 表面技术, 2007; 36: 39)
[8] Rodrigues S N, Gon¸calves I C, Martins M C L, Barbosa M A, Ratner B D. Biomaterials, 2006; 27: 5357
[9] Mitsakakis K, Lousinian S, Logothetidis S. Biomol Eng, 2007; 24: 119.
[10] Huang Y, Xiaoying L, Qian W, Tang Z, Zhong Y. Acta Biomater, 2010; 6: 2083.
[11] Gray J J. Curr Opin Struct Biol, 2004; 14: 110
[12] Anselme K. Biomaterials, 2000; 21: 667
[13] MacDonald D E, Rapuano B E, Deo N, Stranick M, Somasundaran P, Boskey A L. Biomaterials, 2004; 25: 3135
[14] Cacciafesta P, Humphris A D L, Jandt K D, Miles M J. Langmuir, 2000; 16: 8167
[15] Gon¸calves I C, Martins M C L, Barbosa M A, Ratner B D. Biomaterials, 2005; 26: 3891
[16] Dion I, Baquey C, Candelon B, Monties J. Int J Artif Organs, 1992; 15: 617
[17] Yuan Y, Liu C, Yin M. J Mater Sci: Mater Med, 2008; 19: 2187
[18] Kaelble D H, Moacanin J. Polymer, 1977; 18: 475
[19] Michiardi A, Aparicio C, Ratner B D, Planell J A, Gil J. Biomaterials, 2007; 28: 586
[20] Nyilas E, Ward Jr R. J Biomed Mater Res, 1977; 11: 69
[21] Depalma V, Baier R, Ford J, Gott V, Furuse A. J Biomed Mater Res, 1972; 6: 37 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|