磁场作用下Al-Pb偏晶合金的凝固过程 |
李海丽, 赵九洲 |
中国科学院金属研究所, 沈阳 110016 |
|
SOLIDIFICATION OF Al-Pb MONOTECTIC ALLOY UNDER A STATIC MAGNETIC FIELD |
LI Haili, ZHAO Jiuzhou |
Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
李海丽 赵九洲. 磁场作用下Al-Pb偏晶合金的凝固过程[J]. 金属学报, 2011, 47(1): 81-87.
,
.
SOLIDIFICATION OF Al-Pb MONOTECTIC ALLOY UNDER A STATIC MAGNETIC FIELD[J]. Acta Metall Sin, 2011, 47(1): 81-87.
[1] Liu Y, Guo J J, Jia J. Foundry, 2000; 49: 11
(刘源, 郭景杰, 贾均. 铸造, 2000; 49: 11)
[2] Inoue A, Yano N. J Mater Sci, 1987; 22: 123
[3] Wecker J, Hehnolt R, Schulta L, Samwer K. Appl Phys Lett, 1993; 52: 1985
[4] Kolbe M, Brillo J, Egry I. Microgravity Sci Technol, 2006; 18: 174
[5] Cao C D, Wei B B. J Mater Sci Technol, 2002; 18: 73
[6] Xu J F, Dai F P,Wei B B. Acta Phys Sin, 2007; 56: 3996
(徐锦峰, 代富平, 魏炳波. 物理学报, 2007; 56: 3996)
[7] Guo J J, Liu Y, Su Y Q. Mater Sci Technol, 2002; 18: 1286
[8] Zhao J Z, Kolbe M, Li H L, Gao J R, Ratke L. Metall Mater Trans, 2007; 38A: 1162
[9] Wang C P, Liu X J, Ohnuma I, Kainuma R, Ishida K. Science, 2002; 297: 990
[10] Zhao J Z. Scr Mater, 2006; 54: 247
[11] Zhang L, Wang E G, Zuo X W, He J C. Acta Metall Sin, 2008; 44: 165
(张林, 王恩刚, 左小伟, 赫冀成. 金属学报, 2008; 44: 165)
[12] Yasuda H, Ohnaka I, Fujimoto S. Mater Lett, 2004; 58: 911
[13] Yasuda H, Ohnaka I, Fujimoto S. Scr Mater, 2006; 54: 527
[14] Zhao J Z, Li H L, Wang Q L, Zhao L, He J. Acta Metall Sin, 2009; 45: 1344
(赵九洲, 李海丽, 王青亮, 赵雷, 何 杰. 金属学报, 2009; 45: 1344)
[15] Zuo X W, Wang E G, Han H, Zhang L, He J C. Acta Metall Sin, 2008; 44: 1219
(左小伟, 王恩刚, 韩欢, 张林, 赫冀成. 金属学报, 2008; 44: 1219)
[16] Decarlo J L, Pirich R G. Metall Trans, 1984; 15A: 2155
[17] Chester W. Scr Mater, 2005; 52: 79
[18] Yang S, Liu W J, Jia J. J Mater Sci, 2001; 36: 5351
[19] Yasuda H, Ohnaka I, Kawakami O. ISIJ Int, 2003; 43: 942
[20] He J, Zhao J Z, Li H L, Zhang X F, Zhang Q X. Metall Mater Trans, 2008; 39A: 1174
[21] Li H L, Zhao J Z. Comput Mater Sci, 2009; 46: 1069
[22] Chester W. J Fluid Mech, 1957; 3: 304
[23] Li H L, Zhao J Z, Zhang Q X, He J. Metall Mater Trans, 2008; 39A: 3308 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|