Al对M2高速钢凝固组织的影响*
周雪峰1,*(), 方峰1, 涂益友1, 蒋建清1, 徐辉霞2, 朱旺龙2
1 东南大学江苏省先进金属材料高技术研究重点实验室, 南京 211189
2 江苏省(天工)工模具钢工程技术研究中心, 丹阳 212312
EFFECT OF ALUMINUM ON THE SOLIDIFICATION MICROSTRUCTURE OF M2 HIGH SPEED STEEL
ZHOU Xuefeng1,*(), FANG Feng1, TU Yiyou1, JIANG Jianqing1, XU Huixia2, ZHU Wanglong2
1 Jiangsu Key Laboratory of Advanced Metallic Materials, Southeast University, Nanjing 211189
2 Jiangsu Engineering Research Center of Tool and Die Steel, Tiangong Group, Danyang 212312
引用本文:

周雪峰, 方峰, 涂益友, 蒋建清, 徐辉霞, 朱旺龙. Al对M2高速钢凝固组织的影响*[J]. 金属学报, 2014, 50(7): 769-776.
Xuefeng ZHOU, Feng FANG, Yiyou TU, Jianqing JIANG, Huixia XU, Wanglong ZHU. EFFECT OF ALUMINUM ON THE SOLIDIFICATION MICROSTRUCTURE OF M2 HIGH SPEED STEEL[J]. Acta Metall Sin, 2014, 50(7): 769-776.

全文: PDF(8944 KB)   HTML
摘要: 

采用OM, TEM, SEM, EBSD, XRD等手段, 分析了不同Al加入量(0%, 0.6%, 1.2%)的M2高速钢的铸态组织, 研究了Al对高速钢凝固组织转变特别是共晶碳化物形貌和微观结构的影响规律. 结果表明, M2高速钢铸态组织主要由位错型马氏体和M2C共晶莱氏体组成. 过量Al (1.2%)促进大量铁素体和针状碳化物形成. Al提高了共晶碳化物的分布均匀性, 促进M2C形貌由纤维状转变为片状, 并使碳化物微观结构发生明显改变. 片状碳化物表面平行于(0002)晶面, 内部存在微孪晶、层错等缺陷, 片层之间具有不同的晶体取向, 而纤维状碳化物内部缺陷极少, 呈单晶取向. 与纤维状碳化物相比, 加Al后形成的片状碳化物高温加热时不易团球化, 对碳化物尺寸细化不利. 添加过量Al (1.2%)形成的铁素体无法通过常规热处理消除, 使高速钢淬火硬度显著降低.

关键词 : M2高速钢,  Al,  凝固组织,  M2C共晶碳化物,  微观结构    
Abstract:

The effect of aluminum on the solidification microstructure of M2 high speed steel, particularly the morphology and microstructure of eutectic carbides, has been investigated by OM, TEM, SEM, EBSD and XRD. The results show that the as-cast microstructure consists of dislocation martensite and M2C eutectic ledeburite. Excessive amount of aluminum, 1.2%, favors the formation of ferrite and needle-like carbides. After the addition of aluminum, eutectic carbides are distributed more homogeneously. Additionally, the morphology of M2C eutectic carbides transforms from the fibrous to the plate-like, and their microstructure also changes significantly. The plate-like M2C has crystal defects, such as micro-twins and stacking faults, and different growing orientation between adjacent plates whereas the fibrous carbides have few defects and single crystal orientation. Compared to fibrous carbides, the plate-like carbides are much difficult to get spheroidized at high temperature, which is unfavorable for carbide refinement. The ferrite, formed by adding excessive amount of aluminum, cannot be eliminated by ordinary heat treatments, decreasing remarkably the hardness of high speed steel after quenching.

Key words: M2 high speed steel    aluminum    solidification microstructure    M2C eutectic carbide    microstructure
收稿日期: 2013-09-30     
ZTFLH:  TG142.7  
基金资助:* 国家自然科学基金项目 51301038, 51201031和51371050, 以及江苏省科技成果转化项目 BA2010139 资助
作者简介: null

周雪峰, 男, 1982年生, 讲师, 博士

图1  
图2  
图3  
图4  
图5  
Sample W Mo V Cr Fe
0%Al, FC 33.4 17.2 6.5 5.1 36.4
0.6%Al, PC 39.8 21.6 9.4 5.7 22.5
1.2%Al, PC 42.1 22.3 9.8 5.5 19.3
1.2%Al, NC 40.2 21.2 6.0 4.7 26.8
  
图6  
图7  
图8  
图9  
图10  
[1] Moon H K, Lee K B, Kwon H. Mater Sci Eng, 2008; A474: 328
[2] Wang R, Andren H O, Wisell H, Dunlop G L. Acta Metall Mater, 1992; 40: 1727
[3] Dobrzanski L A, Kasprzak W. J Mater Process Technol, 2001; 109: 52
[4] Liu G L, Zhang G Y, Zeng M G, Qian C F. Chin J Mech Eng, 2002; 38: 149
[4] (刘贵立, 张国英, 曾梅光, 钱存富. 机械工程学报, 2002; 38: 149)
[5] Yang R C, Zhao L M, Wang B, Chen K. Trans Mater Heat Treat, 2009; 30: 185
[5] (杨瑞成, 赵丽美, 王 彬, 陈 奎. 材料热处理学报, 2009; 30: 185)
[6] Xu Z Y. Mater Mech Eng, 1993; 17(2): 4
[6] (徐祖耀. 机械工程材料, 1993; 17(2): 4)
[7] Qian X R, Liu R Y, Liu K. J Chin Electron Microsc Soc, 1986; 3: 151
[7] (钱小蓉, 刘荣运, 刘 可. 电子显微学报, 1986; 3: 151)
[8] Boccalini M, Goldenstein H. Int Mater Rev, 2001; 46: 92
[9] Hetzner D W. Mater Charact, 2001; 46: 175
[10] Liu J T, Chang H B, Wu R H, Hsu T Y, Ruan X Y. Mater Charact, 2000; 45: 175
[11] Fredriksson H, Hillert M, Nica M. Scand J Metall, 1979; 8: 115
[12] Fischmeister H F, Riedl R, Karagoz S. Metall Trans, 1989; A20: 2133
[13] Lee E S, Park W J, Baik K H, Ahn S. Scr Mater, 1998; 39: 1133
[14] Zhou X F, Fang F, Li F, Jiang J Q. J Mater Sci, 2011; 46: 1196
[15] Zhou X F, Fang F, Li G, Jiang J Q. ISIJ Int, 2010; 50: 1151
[16] Li Y J, Jiang Q C, Zhao Y G, He Z M. Scr Mater, 1997; 37: 173
[17] Li Y J, Jiang Q C, He Z M, Zhao Y G, Ge L H. Chin J Mater Res, 1997; 11: 216
[17] (李彦君, 姜启川, 何镇明, 赵宇光, 葛僚海. 材料研究学报, 1997; 11: 216)
[18] Zhao Y Q, Jiang Q C, Zhao Y G, Li Y J, Jiang Z L. J Jilin Univ Technol, 1997; 27: 28
[18] (赵玉谦, 姜启川, 赵宇光, 李彦君, 蒋自力. 吉林工业大学学报, 1997; 27: 28)
[19] Zhou X F, Fang F, Jiang J Q. Foundry Technol, 2009; 30: 160
[19] (周雪峰, 方峰, 蒋建清. 铸造技术, 2009; 30: 160)
[20] Mclaughlin J, Kraft R W, Goldstein J I. Metall Trans, 1977; 8A: 1787
[21] Wu C J,Chen G L,Qiang W J. Metal Science. Beijing: Metallurgical Industry Press, 2003: 3
[21] (吴承建,陈国良,强文江. 金属材料学. 北京: 冶金工业出版社, 2003: 3)
[22] Cui X H, Wang S Q, Wu H, Jiang Q C. J Jilin Univ Technol, 2002; 32: 42
[22] (崔向红, 王树奇, 吴 宏, 姜启川. 吉林工业大学学报, 2002; 32: 42)
[23] Li Y J, Jiang Q C, Zhao Y G, He Z M, Zhong X Y. Acta Metall Sin, 1999; 35: 207
[23] (李彦君, 姜启川, 赵宇光, 何镇明, 钟雪友. 金属学报, 1999; 35: 207)
[1] 马德新, 赵运兴, 徐维台, 王富. 重力对高温合金定向凝固组织的影响[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[3] 孙蓉蓉, 姚美意, 王皓瑜, 张文怀, 胡丽娟, 仇云龙, 林晓冬, 谢耀平, 杨健, 董建新, 成国光. Fe22Cr5Al3Mo-xY合金在模拟LOCA下的高温蒸汽氧化行为[J]. 金属学报, 2023, 59(7): 915-925.
[4] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[5] 王宗谱, 王卫国, Rohrer Gregory S, 陈松, 洪丽华, 林燕, 冯小铮, 任帅, 周邦新. 不同温度轧制Al-Zn-Mg-Cu合金再结晶后的{111}/{111}近奇异晶界[J]. 金属学报, 2023, 59(7): 947-960.
[6] 王福容, 张永梅, 柏国宁, 郭庆伟, 赵宇宏. Al掺杂Mg/Mg2Sn合金界面的第一性原理计算[J]. 金属学报, 2023, 59(6): 812-820.
[7] 冯艾寒, 陈强, 王剑, 王皞, 曲寿江, 陈道伦. 低密度Ti2AlNb基合金热轧板微观组织的热稳定性[J]. 金属学报, 2023, 59(6): 777-786.
[8] 张德印, 郝旭, 贾宝瑞, 吴昊阳, 秦明礼, 曲选辉. Y2O3 含量对燃烧合成Fe-Y2O3 纳米复合粉末性能的影响[J]. 金属学报, 2023, 59(6): 757-766.
[9] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[10] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.
[11] 王迪, 贺莉丽, 王栋, 王莉, 张思倩, 董加胜, 陈立佳, 张健. Pt-Al涂层对DD413合金高温拉伸性能的影响[J]. 金属学报, 2023, 59(3): 424-434.
[12] 李斗, 徐长江, 李旭光, 李双明, 钟宏. La掺杂P型CeyFe3CoSb12 热电材料及涂层的热电性能[J]. 金属学报, 2023, 59(2): 237-247.
[13] 王虎, 赵琳, 彭云, 蔡啸涛, 田志凌. 激光熔化沉积TiB2 增强TiAl基合金涂层的组织及力学性能[J]. 金属学报, 2023, 59(2): 226-236.
[14] 朱智浩, 陈志鹏, 刘田雨, 张爽, 董闯, 王清. 基于不同 α / β 团簇式比例的Ti-Al-V合金的铸态组织和力学性能[J]. 金属学报, 2023, 59(12): 1581-1589.
[15] 巩向鹏, 伍翠兰, 罗世芳, 沈若涵, 鄢俊. 自然时效对Al-2.95Cu-1.55Li-0.57Mg-0.18Zr合金160℃人工时效的影响[J]. 金属学报, 2023, 59(11): 1428-1438.