| 添加Sn粉激光焊接钢/铝合金异种金属的显微组织与性能 |
| 周惦武,彭艳,徐少华,刘金水 |
| 湖南大学汽车车身先进设计制造国家重点实验室, 长沙 410082 |
|
| MICROSTRUCTURE AND MECHANICAL PROPERTY OF STEEL/Al ALLOY LASER WELDING WITH Sn POWDER ADDITION |
| ZHOU Dianwu, PENG Yan, XU Shaohua, LIU Jinshui |
| State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body,Hunan University, Changsha 410082 |
引用本文:
周惦武,彭艳,徐少华,刘金水. 添加Sn粉激光焊接钢/铝合金异种金属的显微组织与性能[J]. 金属学报, 2013, 49(8): 959-968.
ZHOU Dianwu,
PENG Yan,
XU Shaohua,
LIU Jinshui.
MICROSTRUCTURE AND MECHANICAL PROPERTY OF STEEL/Al ALLOY LASER WELDING WITH Sn POWDER ADDITION[J]. Acta Metall Sin, 2013, 49(8): 959-968.
| [1] Lei Z, Wang X Y, Wang W B, Lin S Y. Trans China Weld Inst, 2007; 28(11): 65
(雷振, 王旭友, 王伟波, 林尚杨. 焊接学报, 2007; 28(11): 65)
[2] Torkamany M J, Tahamtan S, Sabbaghzadeh J. Mater Des, 2010; 31: 458
[3] Zhang Q Y, Liu S Q. Acta Metall Sin, 1981; 17: 300
(张启运, 刘淑淇. 金属学报, 1981; 17: 300)
[4] Guo J T, Sun C, Tan M H, Li H, Lai W H. Acta Metall Sin, 1990; 26: 20
(郭建亭, 孙超, 谭明晖, 李辉, 赖万慧. 金属学报, 1990; 26: 20)
[5] Zhang Q X. Rare Met Mater Eng, 1990; 20: 27
(章桥新. 稀有金属材料与工程, 1990; 20: 27)
[6] Wang L G, Zhang B F, Guan S K, Qi X H, Geng J Y. Rare Met Mater Eng, 2007; 36: 59
(王利国, 张保丰, 关绍康, 齐新华, 耿家源. 稀有金属材料与工程, 2007; 36: 59)
[7] Boag A, Hughes A E, Wilson N C, Torpy A, Macrae M C, Glenn A M, Muster T H. Corros Sci, 2009; 51: 1565
[8] Akdeniz M V, Mekhrabov A O. Acta Mater, 1998; 46: 1185
[9] Mathieu A, Pontevicci S, Viala J C, Cicala E, Matte\"{\i S, Grevey D.Mater Sci Eng, 2006; A435-436: 19
[10] Lin S B, Song J L, Yang C L, Fan C L, Zhang D W. Mater Des, 2010; 31: 2637
[11] Braun R. Mater Sci Eng, 2006; A426: 250
[12] Sierra G, Peyre P, Deschaux B F. Mater Charact, 2008; 59: 1705
[13] Segall M D, Lindan P L D, Probert M J, Pickard C J, Hasnip P J, Clark S J,Payne M C. J Phys: Condens Matter, 2002; 14: 2717
[14] Marlo M, Milman V. Phys Rev, 2000; 62B: 2899
[15] White J A, Bird D M. Phys Rev, 1994; 50B: 4954
[16] Lei Z, Yu N, You A Q, Lin S Y. Trans China Weld Inst, 2008; 29(6): 21
(雷振, 于宁, 游爱清, 林尚扬. 焊接学报, 2008; 29(6): 21)
[17] Song J L, Lin S B, Yang C L, Ma G C. Aeronaut Manuf Technol, 2008; 12: 26
(宋建岭, 林三宝, 杨春利, 马广超. 航空制造技术, 2008; 12: 26)
[18] Hao Y L, Xu D S, Cui Y Y, Yang R, Li D. Acta Mater, 1999; 47: 1129
[19] Kobayashi S, Yakou T. Mater Sci Eng, 2002; A338: 44
[20] Simmons G, Wang H. Single Crystal Elastic Constants and Calculated Aggregate Properties. Cambridge: MIT Press, 1971: 80
[21] Fu C L, Yoo M H. Acta Mater, 1992, 40: 703
[22] Kong Y, Hu W Y, Huang Y C, Shu X L. Rare Met Mater Eng, 2003; 32: 87
(孔毅, 胡望宇, 黄杨程, 舒小林. 稀有金属材料与工程, 2003; 32: 87)
[23] Mehl M J, Osburn J E, Papaconstantopoulos D A, Klein B M. Phys Rev,1990; 41B: 10311
[24] Pugh S F. Philos Mag, 1954; 45: 823
[25] Yu W Y, Wang N, Xiao X B, Tang B Y, Peng L M, Ding W J. Solid State Sci,2009; 11: 1400
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|