| DISLOCATION FEATURES IN POLYSYNTHETICALLY TWINNED TiAl CRYSTALS AFTER DEFORMATION AT HIGH TEMPERATURE |
| LIU Yi;LIN Dongliang; WANG Dening; CHEN Da; CHEN Shipu(Shanghai Jiaotong University; Shanghai 200030; State Key Laboratory of Solid State Microstructures; Nanjing University; Nanjing 210008); LIU Zhiguo; MENG Xiangkang (Nanjing University; Nanjing 210008)(Manuscript received 1995-09-07) |
|
Cite this article:
LIU Yi;LIN Dongliang; WANG Dening; CHEN Da; CHEN Shipu(Shanghai Jiaotong University; Shanghai 200030; State Key Laboratory of Solid State Microstructures; Nanjing University; Nanjing 210008); LIU Zhiguo; MENG Xiangkang (Nanjing University; Nanjing 210008)(Manuscript received 1995-09-07). DISLOCATION FEATURES IN POLYSYNTHETICALLY TWINNED TiAl CRYSTALS AFTER DEFORMATION AT HIGH TEMPERATURE. Acta Metall Sin, 1996, 32(5): 456-461.
|
|
|
Abstract The dislocation features in polysynthetically twinned (PST) TiAl crystal deformed at 400, 600 and 850℃ have been investgated by TEM. Screw <011] superdislocations turned to dissociate on {100} planes to form Kear-Wilsdorf locks. Faulted dipoles were found in specimens deformed below 600℃ , whereas no faulted dipole was found at 850℃.In-situ heating observations on the faulted dipoles formed during deformation at room temperature indicated that the faulted dipole disappeared at about 600℃. Based on these experimental results, the mechanism of brittle-to-ductile of TiAl alloy has been discussed.
|
|
Received: 18 May 1996
|
| 1LipsittHA,SchechtmanD,SchafrikRE.MetallTrans,1975;6A:19912YamaguchiM,InuiH.MaterResSocSympProc,1995;364:13刘毅,汪德宁,陈达,林栋梁,刘治国.金属学报,1995,31:3934刘毅,汪德宁,陈达,林栋梁,刘治国,孟祥康.金属学报,1995;32:4495InuiH,OhMH,NakamuraA,YamaguchiM.PhitosMag,1992;66A:5396KearBH,WilsdorfHGE.TransMetallSocAIME,1962;224:3827SchechtmanD,BlackburnMJ,LipsittHA.MetallTrans,1974;54:13738HugG,LoiseanA,Lasalmonie.PhilosMag,1986;54A:479YaoK-F,InuiH,KishidaK,YamaguchiM.ActaMetallMater,1995;43:1075 |