| AN ANALYSIS OF VALENCE ELECTRON STRUCTURE OF Fe-C-Mn ALLOYING AUSTENITE |
| ZHU Ruifu; LU Yupeng; CHEN Chuanzhong; LI Shitong; WANG Shiqing (Shandong University of Technology; Jinan 250061) ZHANG Fucheng (Yanshan University; Qinhuangdao 066004) |
|
Cite this article:
ZHU Ruifu; LU Yupeng; CHEN Chuanzhong; LI Shitong; WANG Shiqing (Shandong University of Technology; Jinan 250061) ZHANG Fucheng (Yanshan University; Qinhuangdao 066004). AN ANALYSIS OF VALENCE ELECTRON STRUCTURE OF Fe-C-Mn ALLOYING AUSTENITE. Acta Metall Sin, 1996, 32(6): 561-564.
|
|
|
Abstract The valence electron structure of Fe-C-Mn alloying austenite containing 1.6% C(mass fraction) has been established by using bond length difference (BLD) method of the empirical electron theory of solids and molecules. The experimental results show that in unit cell containing C and Mn atoms, Fe~c, Fe~f and Mn atoms are on the 16th, 18th and 10th hybrid levels of B-type hybridization states respectively, and the carbon atom is on its 6th hybrid level. The simultaneous increase in C and Mn content will increase the number of the strongest C-Mn bond, thus lead to the increase in austenitic stability and work hardening capacity.
|
|
Received: 18 June 1996
|
| 1余瑞璜.科学通报,1978:23(4):2172刘志林,张瑞林,王斌.中国科学,1989;A(1):923朱瑞富.哈尔滨工业大学博士学位论文,19944余瑞璜,刘志林.金属科学与工艺,1988;7(2):15苏荣浩.兵器材料科学与工程,1985;(12):136张瑞林.固体与分子经验电子理论,长春:吉林科学技术出版社,1993:2347张瑞林,余瑞璜,金属学报,1984;20:A2798宋学孟.金属物理性能分析.北京:机械工业出版社,1990:57 |