Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (10): 1040-1046    DOI:
Current Issue | Archive | Adv Search |
IN SITU INVESTIGATION OF PITTING INITIATION AND PROPAGATION IN SiC_p /2024 Al METAL MATRIX C0MPOSITES
FENG Zude; LIN Changjian;TAN Jianguang (State Key Laboratory for Physical Chemistry of the Solid Surface; Xiamen University; Xiamen 361005) LIN Junshan(Shanghai Jiaotong University; Shanghai 200030)
Cite this article: 

FENG Zude; LIN Changjian;TAN Jianguang (State Key Laboratory for Physical Chemistry of the Solid Surface; Xiamen University; Xiamen 361005) LIN Junshan(Shanghai Jiaotong University; Shanghai 200030). IN SITU INVESTIGATION OF PITTING INITIATION AND PROPAGATION IN SiC_p /2024 Al METAL MATRIX C0MPOSITES. Acta Metall Sin, 1997, 33(10): 1040-1046.

Download:  PDF(1206KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The corrosion characteristics of as-cast SiCp/ 2024 al composites in chloride (Cl-) media were investigated using scanning micro reference electrode technique,electrochemical analysis and scanning electron microscopy. The composites have less resistant to pit initiation than the corresponding aluminum alloy. The increase in volume fraction of SiCp reinforced phase resulted in a signiflcant decrease of pitting potential. In situ mapping of the active centers in composites revealed that local breakdown of passivity and micropitting corrosion could happen even at the open-circuit potentials, and the increase of volume fraction of SiC particles reinforced phase in the composites led t0 a significant increase of active centers on their surfaces. Pitting corrosion attack occured preferentially at the interfaces of SiC / al, and al2Cu or (Cu, Fe, Mn)al6 inclusions / al for the composites.
Key words:  Al-based metal metrix composite      scanning micro reference electrode technique      pitting corrosion      initiation stage     
Received:  18 October 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I10/1040

1 Lucas K a, Clarke H. Corrosion of aluminum-based metal matrix composites. Somerset, England;Research Studies Press Ltd. 1993: 6
2 Sun H, Koo E Y, Wheat H G. Corrosion, 1991. 47; 741
3 Buarzaige M M, Thorpe S J. Corrosion, 1994; 50:176
4 Roper G M, attwood P a. J Maler Sci, 1995, 30:898
5 Nunes P C R, Ramanathan L V. Corrosion, 1995; 51:610
6 Coleman S L, Scott V D, McEnaney B. J Mater Sci, 1994, 29:2826
7 Trowsdale a J, Noble B, Harris S J, Gibbins I S R et al. Corrosion Science, 1996, 38:177
8 Traskoma P P. Corrosion, 1990; 46:402
9 Castle J E, Sun L, Yan H. Corrosion Science, 1994, 36:1093
10 林昌健,厦门大学博士学位论文,1985
11 林君山,李鹏兴,吴人洁,金属学报,1992, 28:B465
12 Trzaskoma P P, McCafferty E, Crowe C R. J Electrochem Soc, 1983, 130:1804
13 Foley R T. Corrosion, 1986; 42:277
14 林昌健,田昭武,物理化学学报,1987, 3; 479
15 Hihara L H, Latanision R M. Corrosion, 1992; 48:546
16 Vogelsang M, arsenault R J, Fisher R M. Metall Trans. 1986; 17a:379
17 arsenault R J, Wang L,Feng C R. acta Metall Mater, 1991, 39:47
18 Mclntyre J F.Conrad R K,Golledge S L.Corrosion 1990; 46:902
19 Hollingsworth E H,Hunsicker H K.Metal Handbook 9th Ed,Vol 13.aSM.1987:583
20 aluminum:properties,physical metallurgy and phase diagrams,Vol.1,In:Van Horn K R ed.Materials Park, OH: aSM International. 1967: 212
[1] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[2] SUN Yangting, LI Yiwei, WU Wenbo, JIANG Yiming, LI Jin. Effect of Inclusions on Pitting Corrosion of C70S6 Non-Quenched and Tempered Steel Doped with Ca and Mg[J]. 金属学报, 2022, 58(7): 895-904.
[3] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[4] LV Chenxi, SUN Yangting, CHEN Bin, JIANG Yiming, LI Jin. Influence of Potentionstatic Pulse Technique on Pitting Behavior and Pitting Resistance of 317L Stainless Steel[J]. 金属学报, 2021, 57(12): 1607-1613.
[5] Kaiqiang LI, Lujia YANG, Yunze XU, Xiaona WANG, Yi HUANG. Influence of SO42- on the Corrosion Behavior of Q235B Steel Bar in Simulated Pore Solution[J]. 金属学报, 2019, 55(4): 457-468.
[6] FENG Hao,LI Huabing,LU Pengchong,YANG Chuntian,JIANG Zhouhua,WU Xiaolei. Investigation on Microbiologically Influenced Corrosion Behavior of CrCoNi Medium-Entropy Alloy byPseudomonas Aeruginosa[J]. 金属学报, 2019, 55(11): 1457-1468.
[7] Nan PIAO,Ji CHEN,Chengjiang YIN,Cheng SUN,Xinghang ZHANG,Zhanwen WU. INVESTIGATION ON PITTING CORROSION BEHAVIOR OF ULTRAFINE-GRAINED 304L STAINLESS STEEL IN Cl- CONTAINING SOLUTION[J]. 金属学报, 2015, 51(9): 1077-1084.
[8] Haiwei HUANG, Zhenbo WANG, Li LIU, Xingping YONG, Ke LU. FORMATION OF A GRADIENT NANOSTRUCTURED SURFACE LAYER ON A MARTENSITIC STAINLESS STEEL AND ITS EFFECTS ON THE ELECTRO- CHEMICAL CORROSION BEHAVIOR[J]. 金属学报, 2015, 51(5): 513-518.
[9] XIN Sensen, LI Moucheng, SHEN Jianian. EFFECT OF TEMPERATURE AND CONCENTRATION RATIO ON PITTING RESISTANCE OF 316L STAINLESS STEEL IN SEAWATER[J]. 金属学报, 2014, 50(3): 373-378.
[10] WANG Binbin, WANG Zhenyao, CAO Gongwang, LIU Yanjie, KE Wei. LOCALIZED CORROSION OF ALUMINUM ALLOY 2024 EXPOSED TO SALT LAKE ATMOSPHERIC ENVIRONMENT IN WESTERN CHINA[J]. 金属学报, 2014, 50(1): 49-56.
[11] SUN Feilong, LI Xiaogang, LU Lin, CHENG Xuequn, DONG Chaofang, GAO Jin. CORROSION BEHAVIOR OF 5052 AND 6061 ALUMINUM ALLOYS IN DEEP OCEAN ENVIRONMENT OF SOUTH CHINA SEA[J]. 金属学报, 2013, 49(10): 1219-1226.
[12] WEI Xin, DONG Junhua, TONG Jian, ZHENG Zhi,KE Wei. INFLUENCE OF TEMPERATURE ON PITTING CORROSION RESISTANCE OF Cr26Mo1 ULTRA PURE HIGH CHROMIUM FERRITE STAINLESS STEEL IN 3.5%NaCl SOLUTION[J]. 金属学报, 2012, 48(4): 502-507.
[13] GUO Lifang LI Xuyan SUN Tao XU Juliang LI Jin JIANG Yiming . THE INFLUENCE OF SENSITIVE TEMPERATURE ON THE LOCALIZED CORROSION RESISTANCE OF DUPLEX STAINLESS STEEL SAF2304[J]. 金属学报, 2012, 48(12): 1503-1509.
[14] ZHOU Binghai ZHAI Ziqing. STOCHASTIC PROCESS-BASED MODELING METHOD FOR PITTING CORRSION OF Ni-BASED ALLOY 690[J]. 金属学报, 2011, 47(9): 1159-1166.
[15] SHI Jinjie SUN Wei GENG Guoqing. CORROSION RESISTANCES OF PASSIVE FILMS ON LOW-CARBON REBAR AND FINE-GRAINED REBAR IN ALKALINE MEDIA[J]. 金属学报, 2011, 47(4): 449-454.
No Suggested Reading articles found!