| MARTENSITE IN U-10%Zr ALLOY |
| XIE Guoqiang; CHU Fengmin. YANG Jilian; LI Wendan; ZHANG Baisheng (China Institute of Atomic Energy; P. O.Box 275(51); BeiJing 102413) (Manuscript received 1996-09-09; in revised form 1996- 11 -22) |
|
Cite this article:
XIE Guoqiang; CHU Fengmin. YANG Jilian; LI Wendan; ZHANG Baisheng (China Institute of Atomic Energy; P. O.Box 275(51); BeiJing 102413) (Manuscript received 1996-09-09; in revised form 1996- 11 -22). MARTENSITE IN U-10%Zr ALLOY. Acta Metall Sin, 1997, 33(8): 785-790.
|
|
|
Abstract The martensitic phases and their structure of the heat treated U- 10%Zr alloy have been studied. The α′ martensite phase with orthorhombic structure and the high plastici-ty α″ martensite phase with monoclinic form can be obtained by water-quenching and an-nealing in γ single phase section or γl+γ2 miscibility gap and β+γ2 or α+γ2 phase section, respectively. Owing to forming martensite phase, both the hardness of the sample and the lat-tice parameters of α phase will be changed.
|
|
Received: 18 August 1997
|
1杨洪广,李文.核科学与工程,1995;15(4):106 2 Xie G Q, Yang J L, Zhang B S, Li W D. Acta Metall Sin (Engl Lett), 1995, 8(3):174 3 Zegler S T. US AEC Rep, ANL-6055, Argonne National Laboratory, 1962:1 4 Wilkinson W D. Uranium Metallurgy. Vol II, New York: Interscience Publishers, 1962:1128 5 D'Amato C, Saraceno F S, Wilson T B. J Nucl Mater, 1964; 12(3): 291 6 Eckelmcyer K H. Metall Trans. 1984; 15A: 1319 7 Tangri K, Williams G I. J Nucl Mater, 1961; 4(2): 226 8 Lagerberg G. J Nucl Mater, 1963, 9(3). 261x |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|