EFFECT OF COATINGS ON OXIDAfION RESISTANCE AND MECHANICAL PROPERTIES OF Ti60 ALLOY
TANG Zhaolin;WANG Fuhui; WANG Qingjiang; WU Weitao; LI Dong (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015 Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

TANG Zhaolin;WANG Fuhui; WANG Qingjiang; WU Weitao; LI Dong (State Key Laboratory for Corrosion and Protection; Institute of Corrosion and Protection of Metals; The Chinese Academy of Sciences; Shenyang 110015 Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). EFFECT OF COATINGS ON OXIDAfION RESISTANCE AND MECHANICAL PROPERTIES OF Ti60 ALLOY. Acta Metall Sin, 1998, 34(3): 325-331.

Download:  PDF(3916KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of several sputtered coatings on oxidation resistance and mechanical properties of Ti60 alloy was investigated. Sputtered pure Al, Ti-36Al, Ni-16Cr-2.SAl (mass fraction, %) coatings and reactively-sputtered Al2O3 film were effective in decreasing the oxidation rate of Ti60 alloy. Al2O3 and TiAl coatings exhibited a better effect than Al and NiCrAl coatings from the point of view of coating compatiability to substrate. The tensile test after 100 h exposure at 600℃ in air also showed that Ti60 alloy with Al2O3 and Toil coatings exhibited a higher ductility than that with Al and NiCrAl coatings. TiAlCr coating exhibits a better combination of oxidation resistance and compatiability to substrate than the above investigated coatings.
Key words:  Ti60 alloy      okidation      coating      thermal stability     
Received:  18 March 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I3/325

1Unnam Jg Shenoy R N, Clark R K. Oxid Met, 1986; 26: 231
2Clark R K, Unnam J. TMS-AIME Paper,No.A84-571 TMS-AIME Annual Meeting,Los Angeles, 1984
3张亚明,周龙江,王卫林,李铁藩,陈崇伟稀有金属材料与工程,1993;22(1):27(Zhang Yaming, Zhou Lonaiiang, Wang Weilin, Li Tiefan, Chen ChongWwei.Rare Met Mater Eng,1993;22:27)
4Streiff R,Poize S.In:Rapp R A ed., High Temperature Corrosion,NACE-6,Houston,1983:591
5Clark R K,Unnaam J,Widemann K E.Oxid Met,1987;28:391
6McKee D W, Luthra L. Surf Coat Technol, 1993; 56: 109
7BenienH;Maushart J,Meter M,Suchentruck R.Mater Sci Eng,1991;A139:126
8王福会,李东,吴维,胡壮麒.金属学报,1995;31(Suppl):S602(Wang Fuhui, Li Dong, Wu Weitao, Hu Zhuangqi. Acta Metall Sin; 1995; 31(Suppl):S602)
9唐兆麟,王福会,吴维.金属学报,1997;33:1028(Tang Zhaolin, Wang Fuhui; Wu Weitao. Acta Metall Sin, 1997; 33: 1028
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[3] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[4] FENG Li, WANG Guiping, MA Kai, YANG Weijie, AN Guosheng, LI Wensheng. Microstructure and Properties of AlCo x CrFeNiCu High-Entropy Alloy Coating Synthesized by Cold Spraying Assisted Induction Remelting[J]. 金属学报, 2023, 59(5): 703-712.
[5] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
[6] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[7] WANG Di, HE Lili, WANG Dong, WANG Li, ZHANG Siqian, DONG Jiasheng, CHEN Lijia, ZHANG Jian. Influence of Pt-Al Coating on Tensile Properties of DD413 Alloy at High Temperatures[J]. 金属学报, 2023, 59(3): 424-434.
[8] LI Dou, XU Changjiang, LI Xuguang, LI Shuangming, ZHONG Hong. Thermoelectric Properties of P-Type CeyFe3CoSb12 Thermoelectric Materials and Coatings Doped with La[J]. 金属学报, 2023, 59(2): 237-247.
[9] CONG Hongda, WANG Jinlong, WANG Cheng, NING Shen, GAO Ruoheng, DU Yao, CHEN Minghui, ZHU Shenglong, WANG Fuhui. A New Design Inorganic Silicate Composite Coating and Its Oxidation Behavior at High Temperature in Steam Atmosphere[J]. 金属学报, 2022, 58(8): 1083-1092.
[10] ZHAO Xiaofeng, LI Ling, ZHANG Han, LU Jie. Research Progress in High-Entropy Alloy Bond Coat Material for Thermal Barrier Coatings[J]. 金属学报, 2022, 58(4): 503-512.
[11] FENG Kai, GUO Yanbing, FENG Yulei, YAO Chengwu, ZHU Yanyan, ZHANG Qunli, LI Zhuguo. Microstructure Controlling and Properties of Laser Cladded High Strength and High Toughness Fe-Based Coatings[J]. 金属学报, 2022, 58(4): 513-528.
[12] WANG Haowei, ZHAO Dechao, WANG Mingliang. A Review of the Corrosion Protection Technology on In SituTiB2/Al Composites[J]. 金属学报, 2022, 58(4): 428-443.
[13] ZHANG Shihong, HU Kai, LIU Xia, YANG Yang. Corrosion-Erosion Mechanism and Research Prospect of Bare Materials and Protective Coatings for Power Generation Boiler[J]. 金属学报, 2022, 58(3): 272-294.
[14] REN Yuan, DONG Xinyuan, SUN Hao, LUO Xiaotao. Oxide Cleaning Effect of In-Flight CuNi Droplet During Atmospheric Plasma Spraying by B Addition[J]. 金属学报, 2022, 58(2): 206-214.
[15] NIE Jinfeng, WU Yuli, XIE Kewei, LIU Xiangfa. Microstructure and Thermal Stability of Heterostructured Al-AlN Nanocomposite[J]. 金属学报, 2022, 58(11): 1497-1508.
No Suggested Reading articles found!