| PROPERTIES AND ABRASION WEAR RESISTANCE OF AN Al_2O_3-TiC-Co MODIFIED CERAMIC |
| LI Jian; MAO Dongsheng; HUANG Liping; GUO Shaoyi; MAO Zhiyuan(Department of Materials Science and Engineering; Zhejiang University Hangzhou 310027Ion Beam Laboratory; Shanghai Institute of Metallurgy The Chinese Academy of Sciences; Shanghai 200050) |
|
Cite this article:
LI Jian; MAO Dongsheng; HUANG Liping; GUO Shaoyi; MAO Zhiyuan(Department of Materials Science and Engineering; Zhejiang University Hangzhou 310027Ion Beam Laboratory; Shanghai Institute of Metallurgy The Chinese Academy of Sciences; Shanghai 200050). PROPERTIES AND ABRASION WEAR RESISTANCE OF AN Al_2O_3-TiC-Co MODIFIED CERAMIC. Acta Metall Sin, 1998, 34(3): 332-336.
|
|
|
Abstract Ceramic powders of Al2O3 and TiC are coated with a layer of cobalt. Successfully the hot-pressed Al2O3-TiC-Co(ATC) modified ceramic possesses improved mechanical properties. Especially its bending strength and fracture toughness are much higher than that of Al2O3-TiC (AT30) ceramic. The abrasion wear behaviour, mechanisms and wear resistance of ATC and AT30 ceramics are compared and studied. The results show that ATC ceramic possesses driproved wear resistance.
|
|
Received: 18 March 1998
|
1Culter R A, Hurford A C. Mate, Set Eng, 1988; A105/106: 183 2郭绍义,毛志远,郦剑,牟军浙江大学学报,1995;4:488(Gu Shaoyi,Mao Zhiyuan, Li Jian,Mou Jun. J Zhejiang Uni,1995; 4:488 3Wahi R Pt llscbner B.J Mater, Sci,1980; 15: 875 4Lee M,Boron M P.Adv Ceram Mater,1988; 3:183 5Guo S Y,Mao Z Y,Li J,Mou J.In:The 2nd Pacific Rim Int Conf on Materials,Seoul,Koear,1995:2737 6Gabr K H Z. Met Prog,1979; 116: 123 7Evans A G.Wear, of Materials. Metals Park, Ohio: ASM, 1981: 439 8Mou J, Mao Z Y, Li J, Guo S Y.Wear,1995:181—183:194L |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|