| RAPID DIRECTIONAL SOLIDIFICATION OF Al-Pb ALLOY UNDER A STATIC MAGNETIC FIELD |
| ZHAO Jiuzhou; LI Haili; WANG Qingliang; ZHAO Lei; HE Jie |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
ZHAO Jiuzhou LI Haili WANG Qingliang ZHAO Lei HE Jie. RAPID DIRECTIONAL SOLIDIFICATION OF Al-Pb ALLOY UNDER A STATIC MAGNETIC FIELD. Acta Metall Sin, 2009, 45(11): 1344-1348.
|
|
|
Abstract The effect of a static magnetic field on the solidification of monotectic alloy has attracted great attentions. But up to date little is known about the details of the magnetic field influences on the microstructure development during the solidification of a monotectic alloy. In this paper, rapid directional solidification experiments are carried out with Al-Pb alloys under a static magnetic field. The dependence of the solidification microstructure on the intensity of the magnetic field is investigated. The mechanism through which the magnetic field affects the microstructure formation is analyzed. It is indicated that the static magnetic field causes only a small decrease in the Marangoni migration velocity and the Stokes settlement velocity of the minority phase droplets during the liquid-liquid decomposition. Such a small change in the moving velocity of the droplets has only a negligible effect on the microstructure formation. The static magnetic field can suppress the convection efficiently. It enhances the spatial homogeneity of the liquid-liquid phase transformation along the radial direction of the sample, reduces the collision and coagulation frequency between the minority phase droplets and, therefore, causes a decrease in the largest and average sizes of the Pb-rich particles in the solidified sample as well as in the width of the particles size distribution. A static magnetic field is favorable for obtaining a monotectic alloy with well dispersed microstructure.
|
|
Received: 07 May 2009
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.50771097 and 50671111) |
| [1] Zhao J Z, Ratke L. Z Metallkd, 1998; 89: 241
[2] Zhao J Z, Ratke L. Scr Mater, 1998; 39: 181
[3] Liu Y, Guo J J, Jia J, Su Y Q, Ding H S. Acta Metall Sin, 2001; 9: 917
(刘源, 郭景杰, 贾均, 苏彦庆, 丁宏升. 金属学报, 2001; 9: 917)
[4] Wang N, Wei B B. Mater Sci Eng, 2003; A345: 145
[5] Zhao J Z. Acta Metall Sin, 2002; 38: 525
(赵九洲. 金属学报, 2002; 38: 525)
[6] Zhao J Z, Ratke L, Jia J, Li Q C. J Mater Sci Technol, 2002; 18: 197
[7] Guo J J, Cui H B, Su Y Q, Bi W S, Jia J, Fu H Z. Spec Cast Nonferrous Alloys, 2004; 1: 1
(郭景杰, 崔红保, 苏彦庆, 毕维生, 贾 均, 傅恒志. 特种铸造及有色合金, 2004; 1: 1)
[8] Decarlo J L, Pirch R G. Metall Trans, 1984; 15A: 2155
[9] Foner S, Meniff E. Rev Sci Instr, 1968; 139: 171
[10] He J, Zhao J Z, Li H L, Zhang X F, Zhang Q X. Metall Mater Trans, 2008; 39A: 1174
[11] Zhang L, Wang E G, Zuo X W, He J C. Acta Metall Sin, 2008; 44: 165
(张林, 王恩刚, 左小伟, 赫冀成, 金属学报, 2008; 44: 165)
[12] Yasuda H, Ohnaka I, Fujimoto S. Mater Lett, 2004; 58: 911
[13] Yasuda H, Ohnaka I, Fujimoto S. Scr Mater, 2006; 54: 527
[14] Chester W. J Fluid Mech, 1957; 3: 304 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|