| HEAT TREATMENT OF HIGH SPEED STEEL USED FOR CENTRIFUGAL CAST ROLLS |
| LUAN Yikun; BAI Yunlong; SONG Nannan; KANG Xiuhong; LI Dianzhong |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
LUAN Yikun BAI Yunlong SONG Nannan KANG Xiuhong LI Dianzhong. HEAT TREATMENT OF HIGH SPEED STEEL USED FOR CENTRIFUGAL CAST ROLLS. Acta Metall Sin, 2009, 45(4): 470-475.
|
|
|
Abstract DSC and dilatometry were carried out to determine the phase transformation temperature of a high speed steel used for centrifugal cast rolls. Based on the critical transformation temperature, high speed steel was annealed, quenched and tempered in order. The results show that the as–cast high speed steel softens only when annealed at above 630℃ as to be easily machined. Before and after heat treatment, there are only little ifferences between the components, morphologies and contents of MC eutectic carbide. However, more and more metastable M2C eutectic carbides decompose with the increase of quenching temperature; the tempering temperature affects much onthe final hardness of the high speed steel. A relationship between tempering temperature and the secondary hardening is given and the peak temperature of the secondary hardening is determined. And the effects of resolving and precipitating of secondary carbides on the microstructure and properties were also studied.
|
|
Received: 26 June 2008
|
|
|
| Fund: Supported by the Action Plan for Revitalizing Northeast of Chinese Academy of Science (No.DBZX–1–010) |
| [1] Hwang K C, Lee S, Lee H C. Mater Sci Eng, 1998; A254: 282
[2] Park JW, Lee H C, Lee S. Metall Mater Trans, 1999; 30A: 399
[3] Wei S Z, Zhu J H, Xu L J. Mater Sci Eng, 2005; A404: 138
[4] Rodenburg C, RainforthWM. Acta Mater, 2007; 55: 2443
[5] Wang C A. Heavy Castings and Forgings, 2003; (4): 55
(汪长安. 大型铸锻件, 2003; (4): 5)
[6] Xu L J, Xing J D, Wei S Z, Zhang Y Z, Long R. Mater Design, 2007; 28: 1425
[7] Gai Z P. PhD Thesis, Wuhan University of Science and Technology, Wuhan, 2006
(甘宅平. 武汉科技大学博士学位论文, 武汉, 2006)
[8] Hashimoto M, Kubo O, Matsubara Y. ISIJ Int, 2004; 44:372
[9] Leskovsek V, Ule B, Liscic B. J Mater Process Technol, 2002; 127: 298
[10] Han Y J, Li Y Q. Heat Treat Met Abroard, 2001; 22(3): 28
(韩云杰, 李艳秋. 国外金属热处理, 2001; 22(3): 28)
[11] Zhou T H, Ma S J. Heat Treat Met, 1999; 24(5): 15
(周体和, 马素娟. 金属热处理, 1999; 24(5): 15)
[12] Zhou H, Wang J G, Jia S S, Ogi K. Acta Metall Sin, 1997:33: 838
(周宏, 王金国, 贾树盛, 大城桂作. 金属学报, 1997; 33: 838) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|